Summary

Introduction

Chapters 3 and 5 describe the information levels of XPS and SSIMS, respectively. The two techniques are highly complementary, having certain shared attributes but differing markedly in other aspects. XPS detects all elements except hydrogen, is inherently quantitative but has limited sensitivity (typically 0.2 atomic % detection limit for low photoelectron cross-section elements) whereas SSIMS detects all elements with isotope specificity (but some, notably nitrogen, only in combined ions), is inherently difficult to quantify but can have very high sensitivity (ppm of one monolayer). Structural information in XPS is dominated by functionality and limited by the poor dynamic range of chemical shifts whereas SSIMS has a high level of molecular specificity and can discriminate molecular from macromolecular entities. XPS typically has a sampling depth of ∼5nm but in certain circumstances this can be varied and reduced to ∼1 nm. The SSIMS sampling depth is essentially fixed and corresponds to the outermost monolayer. Both techniques are capable of analysing small areas of the order of 50 μm width/diameter and of imaging with reasonable spatial resolution (XPS ~ 10 μm, SSIMS ~ 1 μm under typical conditions). From this it is clear, even in principle, that combining information from the two techniques will be beneficial.

In the early days of SSIMS, when the instrumentation was based on compact quadrupole mass spectrometers, combination XPS/SSIMS systems were popular. Both techniques could be used to examine a sample sequentially in a costeffective way (only one vacuum system is needed and there are no uncertainties about comparing information from discrete samples). As the instrumentation has evolved in complexity (especially with ToF SIMS) stand-alone systems have become the norm.

Information

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Book purchase

Temporarily unavailable

Save book to Kindle

To save this book to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

  • Polymer surface analysis case studies
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.007
Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

  • Polymer surface analysis case studies
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.007
Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

  • Polymer surface analysis case studies
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.007
Available formats
×