Skip to main content Accessibility help
×
Hostname: page-component-7b7567c8c-wxvwp Total loading time: 0 Render date: 2026-11-16T05:01:41.475Z Has data issue: false hasContentIssue false

Chapter 2 - XPS

Published online by Cambridge University Press:  08 October 2009

D. Briggs
Affiliation:
Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
Get access

Summary

Instrumentation

XPS involves the irradiation of a sample with soft X-rays and the energy analysis of photoemitted electrons which are generated close to the sample surface. An X-ray photoelectron spectrometer (or XPS instrument) therefore consists of: a vacuum vessel with its associated pumping system and sample introduction/manipulation systems; an X-ray source; an electron energy analyser and its associated input (or transfer) electron–optical lens; an electron detection system and a dedicated ‘datasystem’ based on a PC or workstation which both controls the spectrometer operation and provides the means to process the acquired data. These components are now considered in turn.

Vacuum system

A comprehensive electron spectrometer vacuum system of typical early 1980s design is illustrated in Fig. 2.1. The spherical analysis chamber allows several probes and analysers to be mounted so that several surface spectroscopies can be applied to the same sample. The construction is mostly of stainless steel with joints made by compressing knife-edge flanges against copper gaskets. In XPS it is important to screen electron trajectories from the earth's magnetic field and this is achieved either by fabricating the analyser chamber and electron analyser/lens vessels out of a material with a high magnetic permeability, usually mu-metal, or by cladding the steel vessel with mu-steel sheeting (internally or externally).

In order for electrons to reach the analyser without being scattered by residual gas molecules, the achievable vacuum only needs to be about 10-5 Torr (1.33 X 10-3Pa), i.e. in the high vacuum regime. However, most vacuum systems routinely operative in the UHV regime (<10-9Torr) in order to reduce the contamination of sample surfaces by absorbed residual gas molecules.

Information

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Book purchase

Temporarily unavailable

Save book to Kindle

To save this book to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

  • XPS
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.003
Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

  • XPS
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.003
Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

  • XPS
  • D. Briggs, Wilton Materials Research Centre, ICI Chemicals and Polymers Ltd
  • Book: Surface Analysis of Polymers by XPS and Static SIMS
  • Online publication: 08 October 2009
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525261.003
Available formats
×