Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-16T08:40:12.401Z Has data issue: false hasContentIssue false

Residual Strains in Al2O3/SiC (Whisker) Composite from 25-1000°C

Published online by Cambridge University Press:  06 March 2019

Benjamin Ballard
Affiliation:
Engineering Department, University of Denver, Denver, CO
Paul Predecki
Affiliation:
Engineering Department, University of Denver, Denver, CO
Camden Hubbard
Affiliation:
HTML, Oak Ridge National Laboratory, Oak Ridge, TN
Get access

Abstract

Residual strains in a hot-pressed α-Al2O3/25 wt % β-SiC (whisker) composite were determined at temperatures from 25 to 1000°C in 250°C increments. The data collected from the (146) reflections of Al2O3 and the (511+333) reflections of SiC whiskers indicates that residual strains in both phases decrease linearly with temperature; the composite's extrapolated zero-strain temperature is determined to be 1471°C and comparable to the value ~1350 °C obtained by Majumdar et al. from neutron data. The lattice thermal expansion of the whiskers agrees well with literature, data for the monolithic β-SiC form.

Information

Type
IX. Nonambient Application of Diffraction
Copyright
Copyright © International Centre for Diffraction Data 1990

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable