Dehydration behaviour of hexadecyltrimethylammonium-exchanged smectite

Published online by Cambridge University Press:  09 July 2018

Abstract

The dehydration of hexadecyltrimethylammonium (HDTMA)-exchanged smectites has been studied using X-ray diffractometry (XRD) and differential scanning calorimetry (DSC). The basal spacing of hydrated HDTMA-smectites changed with temperature. The 2.5 HDTMA-smectite (i.e. smectite treated with HDTMA equivalent to 2.5 times the CEC) showed a continuous increase in its basal spacing during dehydration up to 200ºC, while the 1.2 HDTMA-smectite showed a significant decrease in basal spacing. It is assumed that the less ordered alkyl chains in the wet state in the interlayer region may be rearranged to ordered chains (e.g. all-trans conformation) during sequential dehydration. This results in a decrease in interlayer spacing in the phase with low organic packing density and a flat-lying array (i.e. 1.2 HDTMA-smectite), and a gradual increase in the basal spacing when the chains have a vertical configuration (2.5 HDTMA-smectite).

Information

Type
Research Article
Copyright
Copyright © The Mineralogical Society of Great Britain and Ireland 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable