Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-16T18:00:26.665Z Has data issue: false hasContentIssue false

Hydrothermal reactivity of K-smectite at 300°C and 100 bar: dissolution-crystallization process and non-expandable dehydrated smectite formation

Published online by Cambridge University Press:  09 July 2018

R. Mosser-Ruck
Affiliation:
Université Henri Poincaré-UMR 7566, BP239, 54 Vandoeuvre-lès-Nancy Cedex
M. Cathelineau
Affiliation:
Université Henri Poincaré-UMR 7566, BP239, 54 Vandoeuvre-lès-Nancy Cedex
A. Baronnet
Affiliation:
CNRS-CRMC2, Campus Luminy, Case 913, 13298 Marseille, Cedex
A. Trouiller
Affiliation:
ANDRA, Parc de la Croix Blanche, 1-7 rue Jean Monnet, 92298 Chatenay-Malabry Cedex, France

Abstract

The hydrothermal reactivity of a smectite saturated with K was studied experimentally at 300°C and 100 bar in (Na,K) chloride solutions (Na/K = 0, 50 and 100, liquid/solid ratio = 10/1). X-ray diffraction, TEM and microprobe results show: (1) a partial to total dissolution of the initial smectite layers; and (2) the crystallization of newly-formed euhedral I-S. Random I-S is formed after 7 days, but an ordered mixed-layer I-S containing <30% expandable layers formed in the longest runs (112 days). The I-S is characterized by non-expandable layers of two distinct types: dehydrated smectite and illite. The Si content is lower in the I-S than in the initial smectite, thus creating a charge deficit, mostly compensated by the introduction of Na to the interlayer space, and yielding a silica release to the solution and subsequent crystallization of quartz and cristobalite.

Information

Type
Research Article
Copyright
Copyright © The Mineralogical Society of Great Britain and Ireland 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable