Hostname: page-component-7b7567c8c-2n9c9 Total loading time: 0 Render date: 2026-11-19T06:55:27.526Z Has data issue: false hasContentIssue false

Conversion of chrysotile to a magnesian smectite

Published online by Cambridge University Press:  01 January 2024

Michael Cheshire*
Affiliation:
Texas Tech University, Department of Geosciences, Lubbock, TX 79419, USA
Necip Gũven
Affiliation:
Texas Tech University, Department of Geosciences, Lubbock, TX 79419, USA
*
*E-mail address of corresponding author: Michael.Cheshire@oildri.com
Rights & Permissions [Opens in a new window]

Abstract

Core share and HTML view are not available for this content. However, as you have access to this content, a full PDF is available via the 'Save PDF' action button.

Chrysotile from Thetford Mines in Quebec, Canada was treated first with mild formic or oxalic acid at concentrations of 0.5 to 2.0 N at 200°C in Teflon-lined 12.0 mL Parr bombs. The reaction products were identified by X-ray diffraction as a poorly crystalline Fe-bearing kerolite-like 2:1 layer silicate (which will be described as a kerolitic precipitate or a kerolitic mesophase in this report). Electron microscopic examination showed a thin foily morphology for this kerolitic mesophase that may have formed by the following reaction:(1)

$\mathop {{\rm{M}}{{\rm{g}}_{\rm{6}}}{\rm{S}}{{\rm{i}}_{\rm{4}}}{{\rm{O}}_{{\rm{10}}}}{{\left( {{\rm{OH}}} \right)}_{{8_{\left( {\rm{s}} \right)}}}}}\limits_{{\rm{chrysotile}}} + 6.02{{\rm{H}}^{\rm{ + }}}_{\left( {{\rm{aq}}} \right)} + 0.54{\rm{F}}{{\rm{e}}^{{\rm{2 + }}}}_{\left( {{\rm{aq}}} \right)} \to \mathop {\left( {{\rm{M}}{{\rm{g}}_{{\rm{2}}{\rm{.46}}}}{\rm{Fe}}_{{\rm{0}}{\rm{.54}}}^{{\rm{2 + }}}} \right){\rm{S}}{{\rm{i}}_{\rm{4}}}{{\rm{O}}_{{\rm{10}}}}{{\left( {{\rm{OH}}} \right)}_{\rm{2}}} \cdot n}\limits_{{\rm{kerolitic}}\;{\rm{mesophase}}} {{\rm{H}}_{\rm{2}}}{{\rm{O}}_{\left( {\rm{s}} \right)}} + {\rm{3}}{\rm{.55M}}{{\rm{g}}^{{\rm{2 + }}}}_{\left( {{\rm{aq}}} \right)}$

The magnetite impurity in the initial chrysotile asbestos served as the source of Fe in the above reactions. Subsequently, this kerolitic precipitate was reacted with 0.2 N NaOH for 48–96 h at 200°C and a highly crystalline smectite was formed with the same foily morphology as the kerolitic precipitate. X-ray spectral analyses of the kerolitic mesophase and smectite suggest the following reaction to have taken place:(2)

$\eqalign{ & \mathop {\left( {{\rm{M}}{{\rm{g}}_{{\rm{2}}{\rm{.46}}}}{\rm{Fe}}_{{\rm{0}}{\rm{.54}}}^{{\rm{2 + }}}} \right){\rm{S}}{{\rm{i}}_{\rm{4}}}{{\rm{O}}_{{\rm{10}}}}{{\left( {{\rm{OH}}} \right)}_{\rm{2}}}}\limits_{{\rm{kerolitic}}\;{\rm{mesophase}}} \cdot n{{\rm{H}}_{\rm{2}}}{{\rm{O}}_{\left( {\rm{s}} \right)}} + {\rm{0}}{\rm{.53M}}{{\rm{g}}^{{\rm{2 + }}}}_{\left( {{\rm{aq}}} \right)} + 0.54{\rm{NaO}}{{\rm{H}}_{\left( {{\rm{aq}}} \right)}} + 0.01{\rm{F}}{{\rm{e}}^{{\rm{3 + }}}}_{\left( {{\rm{aq}}} \right)} \to \cr & \;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\;\mathop {\;\;{\rm{N}}{{\rm{a}}_{0.54}}\left( {{\rm{M}}{{\rm{g}}_{{\rm{2}}{\rm{.99}}}}{\rm{Fe}}_{{\rm{0}}{\rm{.01}}}^{{\rm{2 + }}}} \right)\left( {{\rm{S}}{{\rm{i}}_{{\rm{3}}{\rm{.46}}}}{\rm{Fe}}_{{\rm{0}}{\rm{.54}}}^{{\rm{3 + }}}} \right){{\rm{O}}_{10}}{{\left( {{\rm{OH}}} \right)}_{{\rm{2}}\;\left( {\rm{s}} \right)}}}\limits_{{\rm{saponite}}} + 0.54{\rm{S}}{{\rm{i}}^{{\rm{4 + }}}}_{\left( {{\rm{aq}}} \right)} \cr} $

The reaction products, a kerolitic mesophase and smectite, possess a non-fibrous habit in contrast to the fibrous (asbestiform) morphology of chrysotile.

Information

Type
Research Article
Copyright
Copyright © Clay Minerals Society 2005