Multimodal detection and laser-induced damage correlation of real surface defects on fused silica optics

Published online by Cambridge University Press:  24 March 2026

Yubo Liu
Affiliation:
State Key Laboratory of Extreme Photonics and Instrumentation, College of Optical Science and Engineering, Zhejiang University , Hangzhou, ChinaZJU-Hangzhou Global Scientific and Technological Innovation Center , Hangzhou, China
Shiling Wang
Affiliation:
College of Metrology Measurement and Instrument, China Jiliang University , Hangzhou, China
Fengwei Zhang
Affiliation:
State Key Laboratory of Extreme Photonics and Instrumentation, College of Optical Science and Engineering, Zhejiang University , Hangzhou, ChinaZJU-Hangzhou Global Scientific and Technological Innovation Center , Hangzhou, China
Zedong Wang
Affiliation:
ZJU-Hangzhou Global Scientific and Technological Innovation Center , Hangzhou, China
Xiyuan Li
Affiliation:
State Key Laboratory of Extreme Photonics and Instrumentation, College of Optical Science and Engineering, Zhejiang University , Hangzhou, ChinaZJU-Hangzhou Global Scientific and Technological Innovation Center , Hangzhou, China
Lan Wu
Affiliation:
State Key Laboratory of Extreme Photonics and Instrumentation, College of Optical Science and Engineering, Zhejiang University , Hangzhou, ChinaZJU-Hangzhou Global Scientific and Technological Innovation Center , Hangzhou, China
Chong Liu
Affiliation:
State Key Laboratory of Extreme Photonics and Instrumentation, College of Optical Science and Engineering, Zhejiang University , Hangzhou, ChinaZJU-Hangzhou Global Scientific and Technological Innovation Center , Hangzhou, China
Dong Liu*
Affiliation:
State Key Laboratory of Extreme Photonics and Instrumentation, College of Optical Science and Engineering, Zhejiang University , Hangzhou, ChinaZJU-Hangzhou Global Scientific and Technological Innovation Center , Hangzhou, ChinaInstitute of Fundamental and Transdisciplinary Research, Zhejiang University , Hangzhou, China
*
Correspondence to: D. Liu, No. 38, Zheda Road, Xihu District, Hangzhou 310058, China. Email: liudongopt@zju.edu.cn

Abstract

Surface defects on fused silica optics significantly limit their laser-induced damage resistance under ultraviolet pulsed laser irradiation, yet quantitative correlations between defect parameters and damage thresholds remain scarce. This study is the first to perform multimodal detection and correlation analysis of laser-induced damage initiated at real defects on fused silica. Scratches were characterized by scattered light intensity, width and fluorescence intensity, and correlated with the damage-onset fluence (DOF). Results show trailing indent scratches (1.9–8.8 μm wide) have DOFs of 1.27–13.2 J/cm2, while plastic continuous scratches (0.4–5.8 μm wide) exhibit higher DOFs of 12.3– 22.0 J/cm2. Fluorescence intensity strongly negatively correlates with DOF (p < 0.001), as do scratch width and fluorescence intensity at α = 0.01 (p < 0.01). These findings establish scratch width and fluorescence intensity as quantitative damage precursors, advancing surface quality assessment for high-energy laser optics.

Information

Type
Research Article
Creative Commons
Creative Common License - CCCreative Common License - BY
This is an Open Access article, distributed under the terms of the Creative Commons Attribution licence (https://creativecommons.org/licenses/by/4.0), which permits unrestricted re-use, distribution and reproduction, provided the original article is properly cited.
Copyright
© The Author(s), 2026. Published by Cambridge University Press in association with Chinese Laser Press
Figure 0

Figure 1Schematic diagram of the multimodal surface defect detection system.

Figure 1

Figure 2Experimental layout of the laser damage test system.

Figure 2

Figure 3Multimodal characterization of a typical trailing indent scratch: (a) dark-field image; (b) bright-field image; (c) bright-field image after laser irradiation; (d) AFM topography; (e) cross-sectional profile.

Figure 3

Figure 4Multimodal characterization of a typical plastic continuous scratch: (a) dark-field image; (b) bright-field image; (c) bright-field image after laser irradiation; (d) AFM topography; (e) cross-sectional profile.

Figure 4

Figure 5Bright-field images and fluorescence characterization results: (a)–(c) trailing indent scratch; (d)–(f) plastic continuous scratch. (a), (d) Bright-field images. (b), (e) Fluorescence intensity maps. (c), (f) Fluorescence lifetime maps.

Figure 5

Figure 6Comparison of the fluorescence decay curves for the two scratches.

Figure 6

Figure 7Dark-field images of the 12 real scratches on fused silica optics, where (a)–(l) correspond to scratches #1–#12, respectively. Scale bar: 100 μm. The blue circle (200 μm diameter) indicates the laser irradiation spot.

Figure 7

Figure 8Bright-field images of the 12 real scratches on fused silica optics before laser irradiation, where (a)–(l) correspond to scratches #1–#12, respectively. Scale bar: 30 μm.

Figure 8

Figure 9Bright-field images of the 12 real scratches on fused silica optics after laser irradiation, where (a)–(l) correspond to scratches #1–#12, respectively. Scale bar: 30 μm.

Figure 9

Table 1Summary of multimodal detection results and DOFs for real scratches.

Figure 10

Figure 10Plot of the DOF of scratches versus multimodal detection parameters: (a) plot of the DOF of scratches versus dark-field image grayscale value; (b) plot of the DOF of scratches versus scratch width; (c) plot of the DOF of scratches versus fluorescence intensity.

Figure 11

Table 2Critical values of the $t$-distribution (two-tailed, 10 degrees of freedom).

Figure 12

Table 3Statistical analysis of multimodal parameters versus the DOF.