Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-16T15:06:31.533Z Has data issue: false hasContentIssue false

Colloidal processing, surface characterization, and sintering of nano ZrO2 powders

Published online by Cambridge University Press:  03 March 2011

Cihangir Duran
Affiliation:
National Institute of Advanced Industrial Science and Technology, Advanced Sintering Technology Group, Advanced Manufacturing Research Institute, Anagahora 2266-98, Shimoshidami, Moriyama-ku, Nagoya, 463-8560, Japan; and Gebze Institute of Technology, Department of Materials Science and Engineering, 41400, Gebze, Kocaeli, Turkey
Yu Jia
Affiliation:
National Institute of Advanced Industrial Science and Technology, Advanced Sintering Technology Group, Advanced Manufacturing Research Institute, Anagahora 2266-98, Shimoshidami, Moriyama-ku, Nagoya, 463-8560, Japan
Yuji Hotta*
Affiliation:
National Institute of Advanced Industrial Science and Technology, Advanced Sintering Technology Group, Advanced Manufacturing Research Institute, Anagahora 2266-98, Shimoshidami, Moriyama-ku, Nagoya, 463-8560, Japan
Kimiyasu Sato
Affiliation:
National Institute of Advanced Industrial Science and Technology, Advanced Sintering Technology Group, Advanced Manufacturing Research Institute, Anagahora 2266-98, Shimoshidami, Moriyama-ku, Nagoya, 463-8560, Japan
Koji Watari
Affiliation:
National Institute of Advanced Industrial Science and Technology, Advanced Sintering Technology Group, Advanced Manufacturing Research Institute, Anagahora 2266-98, Shimoshidami, Moriyama-ku, Nagoya, 463-8560, Japan
*
a)Address all correspondence to this author. e-mail: y-hotta@aist.go.jp
Get access

Abstract

Colloidally stable suspensions are required to fabricate dense samples with uniform microstructure by colloidal processing methods, which necessitate dispersion of ceramic powders in a liquid medium. Aqueous nano ZrO2 suspensions were prepared using polyethylenimine (PEI) as a dispersant. PEI adsorption on nano ZrO2 surfaces was promoted with increasing initial PEI content and suspension pH. Isoelectric point was shifted from pH 7 at 0 wt% PEI to pH 10.4 at 3 wt% PEI. Stable suspensions had mean particle sizes in the range of 100 to 150 nm and sedimentation rates less than0.4 mm/h, as compared to 2–5.5 μm and 10–50 mm/h for unstable suspensions. Samples with 98% relative density were fabricated after sintering at 1300 °C for 4 h from colloidally stable suspensions.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable