Density- and Hardness-optimized Pressureless Sintered and Post-hot Isostatic Pressed B4C

Published online by Cambridge University Press:  01 August 2005

Namtae Cho
Affiliation:
School of Materials Science and Engineering, Georgia Institute of Technology, Atlanta, Georgia 30332
Zhihao Bao
Affiliation:
School of Materials Science and Engineering, Georgia Institute of Technology, Atlanta, Georgia 30332
Robert F. Speyer*
Affiliation:
School of Materials Science and Engineering, Georgia Institute of Technology, Atlanta, Georgia 30332
*
a) Address all correspondence to this author. e-mail: robert.speyer@mse.gatech.edu
Get access

Abstract

Pressureless sintered B4C relative densities as high as 96.7% were obtained by optimizing the soak temperature, and holding at that temperature for the minimum time required to reach terminal density. Although the relative densities of pressureless sintered specimens were lower than that of commercially produced hot-pressed B4C, their (Vickers) hardness values were comparable. For 4.45-cm-diameter, 1.35-cm-high disk-shaped specimens, pressureless sintered to at least 93.0% relative density, post-hot isostatic pressing resulted in vast increases in relative densities (e.g., 100.0%) and hardness values significantly greater than that of commercially produced hot-pressed B4C.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable