Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-18T07:13:46.064Z Has data issue: false hasContentIssue false

Hardness evolution of Al–Cr–N coatings under thermal load

Published online by Cambridge University Press:  31 January 2011

Herbert Willmann
Affiliation:
Materials Center Leoben, 8700 Leoben, Austria; and Thin Film Physics Division, Department of Physics (IFM), Linköping University, 58183 Linköping, Sweden
Paul H. Mayrhofer*
Affiliation:
Department of Physical Metallurgy and Materials Testing, Montanuniversität Leoben, 8700 Leoben, Austria
Lars Hultman
Affiliation:
Thin Film Physics Division, Department of Physics (IFM), Linköping University, 58183 Linköping, Sweden
Christian Mitterer
Affiliation:
Christian Doppler Laboratory for Advanced Hard Coatings at the Department of Physical Metallurgy and Materials Testing, Montanuniversität Leoben, 8700 Leoben, Austria
*
a)Address all correspondence to this author. e-mail: paul.mayrhofer@unileoben.ac.at
Get access

Abstract

Microstructure and hardness evolution of arc-evaporated single-phase cubic Al0.56Cr0.44N and Al0.68Cr0.32N coatings have been investigated after thermal treatment in Ar atmosphere. Based on a combination of differential scanning calorimetry and x-ray diffraction studies, we can conclude that Al0.56Cr0.44N undergoes only small structural changes without any decomposition for annealing temperatures Ta ⩽ 900 °C. Consequently, the hardness decreases only marginally from the as-deposited value of 30.0 ± 1.1 GPa to 29.4 ± 0.9 GPa with Ta increasing to 900 °C, respectively. The film with higher Al content (Al0.68Cr0.32N) exhibits formation of hexagonal (h) AlN at Ta ⩾ 700 °C, which occurs preferably at grain boundaries as identified by analytical transmission electron microscopy. Hence, the hardness increases from the as-deposited value of 30.1 ± 1.3 GPa to 31.6 ± 1.4 GPa with Ta = 725 °C. At higher temperatures, where the size and volume fraction of the h-AlN phase increases, the hardness decreases to 27.5 ± 1.0 GPa with Ta = 900 °C.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2008

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable