Hostname: page-component-7b7567c8c-2n9c9 Total loading time: 0 Render date: 2026-11-17T07:21:46.426Z Has data issue: false hasContentIssue false

In situ mechanical observations during nanoindentation inside a high-resolution scanning electron microscope

Published online by Cambridge University Press:  31 January 2011

K.A. Rzepiejewska-Malyska*
Affiliation:
Swiss Federal Laboratories for Material Testing and Research—EMPA, CH-3602 Thun, Switzerland
G. Buerki
Affiliation:
Swiss Federal Laboratories for Material Testing and Research—EMPA, CH-3602 Thun, Switzerland
J. Michler
Affiliation:
Swiss Federal Laboratories for Material Testing and Research—EMPA, CH-3602 Thun, Switzerland
R.C. Major
Affiliation:
Hysitron, Inc., Minneapolis, Minnesota 55344
E. Cyrankowski
Affiliation:
Hysitron, Inc., Minneapolis, Minnesota 55344
S.A.S. Asif
Affiliation:
Hysitron, Inc., Minneapolis, Minnesota 55344
O.L. Warren
Affiliation:
Hysitron, Inc., Minneapolis, Minnesota 55344
*
a)Address all correspondence to this author. e-mail: karolina.rzepiejewska@empa.ch
Get access

Abstract

In nanoindentation, the occurrence of cracks, pileup, sink-in, or film delamination adds additional complexity to the analysis of the load–displacement curves. Many techniques and analysis methods have been used to extract both qualitative and quantitative information from the indentation test both during and after the test. Much of this information is obtained indirectly or may even be overlooked by current testing methods (e.g., cracks that open only during the loading cycle of the test may go unnoticed from a typical residual indentation analysis). Here we report on the development of a miniature depth-sensing nanoindentation instrument and its integration into a high-resolution scanning electron microscope. Real-time observation of the nanoindentation test via scanning electron microscopy allows for visualization and detection of certain events such as crack initiation, pileup, or sink-in, and other material deformation phenomena. Initial results from aluminum 〈100〉 and a thin gold film (∼225 nm) are presented.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2008

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable