Lanthanum molybdenum oxide: Low-temperature synthesis and characterization

Published online by Cambridge University Press:  01 May 2006

S. Basu
Affiliation:
Electroceramics Division, Central Glass and Ceramic Research Institute, Kolkata 700 032, India
P. Sujatha Devi*
Affiliation:
Electroceramics Division, Central Glass and Ceramic Research Institute, Kolkata 700 032, India
H.S. Maiti
Affiliation:
Electroceramics Division, Central Glass and Ceramic Research Institute, Kolkata 700 032, India
Y. Lee
Affiliation:
Department of Physics, Brookhaven National Laboratory, Upton, New York 11973
J.C. Hanson
Affiliation:
Department of Chemistry, Brookhaven National Laboratory, Upton, New York 11973
*
a) Address all correspondence to this author. e-mail: psujathadevi@cgcri.res.in
Get access

Abstract

A recently developed fast oxide ion conductor, namely lanthanum molybdenum oxide (La2Mo2O9, LAMO), was synthesized instantaneously by a citrate-nitrate auto-ignition process at a fixed citrate to nitrate ratio of 0.3 and characterized by thermal analysis, x-ray diffraction, impedance spectroscopy, and thermal expansion measurements. Crystalline LAMO has formed instantaneously during the combustion process. The signature of the order–disorder transition of stoichiometric LAMO around 570 °C was evident from differential thermal analysis, differential scanning calorimetry electrical conductivity, and thermal expansion measurements. Though the in situ x-ray measurements did not indicate any clear evidence of a phase transition, a stepwise change in the lattice parameter near the vicinity of the transition temperature was apparent thereby confirming the phase transition to be of first order in nature. The thermal expansion coefficient of LAMO was calculated to be 13.92 × 10−6/°K at 950 °C. The present method formed phase pure LAMO instantaneously and produced sintered samples with high conductivity, namely, 0.052 S/cm at 800 °C and 0.08 S/cm at 950 °C compared to LAMO prepared through various other solution routes.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2006

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable