Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-19T02:58:07.338Z Has data issue: false hasContentIssue false

A note on a common mistake in the analysis of nanoindentation data

Published online by Cambridge University Press:  31 January 2011

M. Munawar Chaudhri
Affiliation:
Cavendish Laboratory, University of Cambridge, Madingley Road, Cambridge CB3 OHE, United Kingdom
Get access

Abstract

It is shown that to analyze the load versus displacement data obtained from a nanoindentation experiment on a flat surface, it is incorrect to use the so called “reduced modulus,” which includes the elastic properties of both the indenter and the test solid. It is suggested that, until correct analytical solutions become available, the indenter should always be of a much stiffer material than the test solid and it should be approximated to a rigid indenter in the analysis. Furthermore, when the indenter and the test surface are of comparable elastic moduli, the measured indenter displacement is the distance of mutual approach of the two contacting bodies rather than the penetration of the indenter below the original surface of the test solid.

Information

Type
Rapid Communications
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable