Hostname: page-component-7b7567c8c-tnkh4 Total loading time: 0 Render date: 2026-11-16T12:19:53.165Z Has data issue: false hasContentIssue false

Oxidation protective barrier coatings for high-temperature polymer matrix composites

Published online by Cambridge University Press:  03 March 2011

David R. Harding
Affiliation:
NASA Lewis Research Center, NYMA, 3001 Aerospace Technology Boulevard, Cleveland, Ohio 44142
James K. Sutter
Affiliation:
NASA Lewis Research Center, 21000 Brookpark Road, Cleveland, Ohio 44135
Marla A. Schuerman
Affiliation:
Xavier University, Cincinnati, Ohio 45207
Elizabeth A. Crane
Affiliation:
John Carroll University, Cleveland, Ohio 44118
Get access

Abstract

Three coating techniques (metal-organic chemical vapor deposition, magnetron sputtering, and plasma-enhanced chemical vapor deposition) were employed to deposit different coating materials (alumina, a superalloy, and silicon nitride) on graphite-fiber-reinforced polyimide composites to protect against oxidation at elevated temperatures. Adhesion and integrity of the coatings were evaluated by isothermal aging (371 °C for 500 h) and thermal cycling (25 to 232 °C for 1000 cycles and −18 to 232 °C for 300 cycles). Best results were achieved with a plasma-deposited, amorphous silicon nitride (a-SiN: H) coating, which withstood stresses from 0.18 to −1.6 GPa. The major factors affecting the suitability of a-SiN: H as an oxidation protective coating are the surface finish of the polymer composite and the presence of a sizable hydrogen content in the coating.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable