Surface analysis of a heat-treated, Al-containing, iron-based superalloy

Published online by Cambridge University Press:  31 January 2011

M. F. López
Affiliation:
Departamento de Corrosión y Protección, Centro Nacional de Investigaciones Metalúrgicas, C.S.I.C., Avda. Gregorio del Amo 8, 28040 Madrid, Spain
A. Gutiéerrez
Affiliation:
Departamento de Corrosión y Protección, Centro Nacional de Investigaciones Metalúrgicas, C.S.I.C., Avda. Gregorio del Amo 8, 28040 Madrid, Spain
M. C. García-Alonso
Affiliation:
Departamento de Corrosión y Protección, Centro Nacional de Investigaciones Metalúrgicas, C.S.I.C., Avda. Gregorio del Amo 8, 28040 Madrid, Spain
M. L. Escudero
Affiliation:
Departamento de Corrosión y Protección, Centro Nacional de Investigaciones Metalúrgicas, C.S.I.C., Avda. Gregorio del Amo 8, 28040 Madrid, Spain
Get access

Abstract

The surface composition of MA 956 superalloy both as-received and after four exposure times at 1100 °C has been investigated by energy dispersive x-ray spectrometry (EDX) and x-ray photoelectron spectroscopy (XPS). The passive layer of the as-received sample is mainly formed by Cr- and Fe-oxides. Heat treatment leads to the formation of an alumina layer on which small nodules grow. XPS spectra evidence the presence of titanium and yttrium oxides at the surface of the heat-treated samples, suggesting Y and Ti outward diffusion through the alumina layer. Iron and chromium oxides at the topmost surface layers are observed only for short heat-treatment times.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable