Surface Effects on Nanoindentation

Published online by Cambridge University Press:  31 January 2011

Tong-Yi Zhang*
Affiliation:
Department of Mechanical Engineering, Hong Kong University of Science and Technology, Clear Water Bay, Kowloon, Hong Kong, China
Wei-Hua Xu
Affiliation:
Department of Mechanical Engineering, Hong Kong University of Science and Technology, Clear Water Bay, Kowloon, Hong Kong, China
*
a)Address all correspondence to this author. e-mail: mezhangt@ust.hk
Get access

Abstract

In this paper, we report on a study of the surface effect on nanoindentation and introduce the apparent surface stress that represents the energy dissipated per unit area of a solid surface in a nanoindentation test. The work done by an applied indentation load contains both bulk and surface work. Surface work, which is related to the apparent surface stress and the size and geometry of an indenter tip, is necessary in the deformation of a solid surface. Good agreement is found between theoretical first-order approximations and empirical data on depth-dependent hardness, indicating that the apparent surface stress plays an important role in depth-dependent hardness. In addition, we introduce a critical indentation depth. The surface deformation predominates if the indentation depth is shallower than the critical depth, while the bulk deformation predominates when the indentation depth is deeper than the critical depth.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable