Amorphization and disordering of the Ni3Al ordered intermetallic by mechanical milling

Published online by Cambridge University Press:  31 January 2011

J. S. C. Jang
Affiliation:
Department of Materials Science and Engineering, North Carolina State University, Box 7907, Raleigh, North Carolina 27695-7907
C. C. Koch
Affiliation:
Department of Materials Science and Engineering, North Carolina State University, Box 7907, Raleigh, North Carolina 27695-7907
Get access

Abstract

The ordered fcc intermetallic compound Ni3Al was mechanically milled in a high energy ball mill. The severe plastic deformation produced by milling induced transformations with increasing milling time as follows: ordered fcc → 2; disordered fcc → 2; nanocrystalline fcc + amorphous. The milling time for complete disordering occurred at 5 h for stoichiometric Ni3Al milled at ambient temperature compared to 50 h for the first observation of an amorphous structure. The structural and microstructural evolution with milling time was followed by x-ray diffraction, TEM, hardness, and calorimetry. The major defect believed responsible for inducing the crystalline-to-amorphous transformation is the fine grain boundary structure with nanometer (∼2 nm diameter) dimensions. The calculated interfacial free energy of the grain boundaries is consistent with the estimated free energy difference between the fcc and amorphous phases in Ni3Al.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 1990

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable