Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-18T03:47:05.485Z Has data issue: false hasContentIssue false

Bulk amorphous Pd–Ni–Fe–P alloys: Preparation and characterization

Published online by Cambridge University Press:  31 January 2011

T. D. Shen
Affiliation:
Materials Science and Technology Division, MS K765, Los Alamos National Laboratory, Los Alamos, New Mexico 87545
Y. He
Affiliation:
Materials Science and Technology Division, MS K765, Los Alamos National Laboratory, Los Alamos, New Mexico 87545
R. B. Schwarz
Affiliation:
Materials Science and Technology Division, MS K765, Los Alamos National Laboratory, Los Alamos, New Mexico 87545
Get access

Abstract

Bulk amorphous alloys of PdxNiyFe80−x−yP20 (25 ≤ x ≤ 60, 20 ≤ y ≤ 55, x + y ≥ 60) were prepared by a flux-melting and water-quenching method. Seven-mm diameter glassy rods of Pd40Ni40−xFexP20 (0 ≤ x ≤ 20) were studied in greater detail. For these alloys, the difference between the crystallization and glass transition temperatures ranges from 102 K for x = 0 to 53 K for x = 20. In this composition range, the reduced glass transition temperature, Trg, ranges from 0.66 to 0.57. The change in density upon crystallization ranges from 0.24 ± 0.04% for x = 0 to 1.33 ± 0.24% for x = 10. The partial molar volume of Fe in amorphous Pd40Ni40−xFexP20 alloys is significantly larger than the molar volume of (metastable) fcc Fe. This, as well as a comparison with the molar volumes of crystalline compounds, suggests chemically selective Fe–Pd bonding in these glasses.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable