Comparative study of nanoindentation on melt-spun ribbon and bulk metallic glass with Ni60Nb37B3 composition

Published online by Cambridge University Press:  23 September 2013

Luis César Rodríguez Aliaga*
Affiliation:
Materials Science and Engineering Department, Federal University of São Carlos, São Carlos, São Paulo, Brazil
Jordina Fornell Beringues*
Affiliation:
Departament de Física, Universitat Autònoma de Barcelona (UAB), 08193 Bellaterra, Barcelona, Spain
Santiago Suriñach
Affiliation:
Departament de Física, Universitat Autònoma de Barcelona (UAB), 08193 Bellaterra, Barcelona, Spain
Maria Dolores Baró
Affiliation:
Departament de Física, Universitat Autònoma de Barcelona (UAB), 08193 Bellaterra, Barcelona, Spain
Claudio Shyinti Kiminami
Affiliation:
Materials Science and Engineering Department, Federal University of São Carlos, São Carlos, São Paulo, Brazil
Claudemiro Bolfarini
Affiliation:
Materials Science and Engineering Department, Federal University of São Carlos, São Carlos, São Paulo, Brazil
Walter José Botta
Affiliation:
Materials Science and Engineering Department, Federal University of São Carlos, São Carlos, São Paulo, Brazil
Jordi Sort Viñas
Affiliation:
Institució Catalana de Recerca i Estudis Avançats and Departament de Física, Universitat Autònoma de Barcelona (UAB), 08193 Bellaterra, Barcelona, Spain
*
a)Address all correspondence to these authors. e-mail: aliaga@ufscar.br

Abstract

This paper describes the mechanical properties under nanoindentation of a new glassy alloy with a nominal composition of Ni60Nb37B3, in the form of melt-spun ribbons and 1-mm-thick copper mold-cast sheets. The alloy composition was designed based on the synergy between the topological instability criterion and the difference in electronegativity among the elements. X-ray diffraction and scanning electron microscopy analyses confirmed that both ribbon and sheet samples possess totally amorphous structures with relatively high thermal stability (supercooled liquid region of about 60 K), as evaluated by differential scanning calorimetry (DSC). Nanoindentation tests revealed that the hardness of this alloy, about 15 GPa, is among the highest reported for metallic glasses. The elastic modulus of the cast sheet is higher and its hardness is similar to that of the ribbon. This correlates well with the different amounts of frozen-in free volume in both types of samples detected by DSC.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2013 
Figure 0

FIG. 1.Synergic effect of topological and chemical factors (λ × Δe) on the Ni–Nb–B ternary system.

Figure 1

FIG. 2.(a) XRD patterns of the melt-spun ribbon and BMG samples of the Ni–Nb–B glassy alloy. (b) BSE-SEM micrographs of the BMG sample.

Figure 2

FIG. 3.(a) DSC curves of the melt-spun ribbon and BMG samples of the Ni–Nb–B glassy alloy subjected to a heating rate of 40 K/min. (b) A comparison of the DSC signal between the ribbon and the sheet indicates the differences in free volume of the two samples.

Figure 3

TABLE I.Thermal parameters determined from DSC measurements at a heating rate of 40 K/min.

Figure 4

FIG. 4.Load–displacement curves obtained by nanoindentation of the ribbon and bulk samples using a Berkovich indenter diamond tip at a constant loading rate of 0.1 mN/s.

Figure 5

FIG. 5.Dependence of hardness, H, and reduced Young's modulus, Er, on the maximum penetration depth during nanoindentation experiments performed on the Ni–Nb–B bulk glassy alloy. The inset shows an indentation imprint performed on the bulk alloy at Pmax = 100 mN.

Figure 6

TABLE II.Mechanical properties determined in nanoindentation tests.

Figure 7

FIG. 6.Experimental and simulated load–unload nanoindentation curves of the Ni-based amorphous alloy measured at a maximum load of 10 mN. Three different numerically simulated P–h curves are shown, using the elastic (Hertz) model, an elastoplastic deformation model based on the conventional Tresca yield criterion, and an elastoplastic model based on the Mohr–Coulomb yield criterion. A good agreement with the experimental curve is obtained in the latter case when a friction coefficient of βM–C = 0.176 and a cohesion of 1.26 GPa are used.

Figure 8

FIG. 7.Circumferential stress (σθθ) contour on the r–z plane developed under the indenter at Pmax = 10 mN, based on the Mohr–Coulomb yield criterion.