Hostname: page-component-7b7567c8c-48dgx Total loading time: 0 Render date: 2026-11-18T05:26:26.194Z Has data issue: false hasContentIssue false

Densification of carbon-rich boron carbide nanopowder compacts

Published online by Cambridge University Press:  18 July 2011

Namtae Cho
Affiliation:
School of Materials Science and Engineering, Georgia Institute of Technology, Atlanta, Georgia 30332
Kathleen G. Silver
Affiliation:
School of Materials Science and Engineering, Georgia Institute of Technology, Atlanta, Georgia 30332
Yolande Berta
Affiliation:
School of Materials Science and Engineering, Georgia Institute of Technology, Atlanta, Georgia 30332
Robert F. Speyer*
Affiliation:
School of Materials Science and Engineering, Georgia Institute of Technology, Atlanta, Georgia 30332
Noel Vanier
Affiliation:
PPG Industries, Inc., Allison Park, Pennsylvania 15101
Cheng-Hung Hung
Affiliation:
PPG Industries, Inc., Allison Park, Pennsylvania 15101
*
a) Address all correspondence to this author. e-mail: robert.speyer@mse.gatech.edu
Get access

Abstract

The densification behavior of 20–40-nm graphite-coated B4C nano-particles was studied using dilatometry, x-ray diffraction, and electron microscopy. The sintering onset temperature was higher than expected from a nanoscale powder (∼1500 °C); remnant B2O3 kept particles separated until B2O3 volatilization, and the graphite coatings imposed particle-to-particle contact of a substance more refractory than B4C. Solid-state sintering (1500–1850 °C) was followed by a substantial slowing of contraction rate attributed to the formation of eutectic liquid droplets more than 10× the size of the original nano-particles. These droplets were induced to form well below the B4C-graphite eutectic temperature by the high surface energy of nanoparticles. They were interpreted to have quickly solidified to form a vast number of voids in particle packing, which in turn, impeded detection of continued solid-state sintering. Starting at 2200 °C, a permanent and interconnected liquid phase formed, which facilitated rapid contraction by liquid phase sintering and/or compact slumping.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable