Effect of particle size and sintering temperature on densification during coupled multifield-activated microforming

Published online by Cambridge University Press:  24 August 2012

Dong Lu
Affiliation:
School of Manufacturing Science and Engineering, Sichuan University, Chengdu, Sichuan 610065, People’s Republic of China
Yi Yang*
Affiliation:
School of Manufacturing Science and Engineering, Sichuan University, Chengdu, Sichuan 610065, People’s Republic of China
Yi Qin
Affiliation:
Department of Design, Manufacture and Engineering Management, Manufacturing Engineering Research Centre, The University of Strathclyde, Glasgow, G1 1XJ, United Kingdom
Gang Yang
Affiliation:
School of Manufacturing Science and Engineering, Sichuan University, Chengdu, Sichuan 610065, People’s Republic of China
*
a)Address all correspondence to this author. e-mail: yangyi0822@yahoo.cn

Abstract

In this paper, a novel sintering method is introduced for the forming of microcomponents in which the loose powders were loaded directly into the die, sintered with an external electric field, a thermal field, and an external stress field (called coupled multifields activation), where the fields were generated by a Gleeble thermal simulation instrument. Two kinds of 316L stainless steel powders of different particle sizes (20 and 70 μm) with no binder were sintered with microforming using a multifield coupling method. For particle size of 20 μm, a nearly fully densified microsintered compact (relative density is 99.2%) was manufactured at a relatively low sintering temperature (900 °C) and within a relatively short sintering time (4 min). The fluctuated temperature–time curve reveals that the rapid mass transfer of liquid phase is the dominant densification mechanism in the compacts with a starting particle size of 20 μm.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2012
Figure 0

FIG. 1.SEM micrographs of the starting 316L stainless steel powders: (a) 20 μm; (b) 70 μm.

Figure 1

TABLE I.Chemical composition of 316L stainless steel (wt%).

Figure 2

FIG. 2.Schematic of Gleeble 1500D apparatus and current distribution.

Figure 3

FIG. 3.The punch and die setup and microsintered compact.

Figure 4

TABLE II.Properties of the powders, processing parameters, and density of the compacts.

Figure 5

FIG. 4.High-resolution SEM images and metallographic photographs of microsintered samples.

Figure 6

FIG. 5.Temperature–time curve of the compacts during the sintering process.

Figure 7

FIG. 6.The effect of sintering temperature on the densification of sintered compacts (20 μm).

Figure 8

FIG. 7.The effect of sintering temperature on the pore distribution of sintered compacts.

Figure 9

FIG. 8.SEM images of compacts with different particle sizes sintered under the same condition (a) welding joints between particles of sample 3#. (b) Particles breakage and deformation of sample 4#.

Figure 10

FIG. 9.Densification of compacts with different starting powder sizes.