Hostname: page-component-7b7567c8c-fvjsw Total loading time: 0 Render date: 2026-11-17T20:25:33.223Z Has data issue: false hasContentIssue false

Effects of angular misalignment on material property characterization by nanoindentation with a cylindrical flat-tip indenter

Published online by Cambridge University Press:  19 December 2016

Naureen B. Shahjahan
Affiliation:
Department of Mechanical Engineering, South Dakota State University, Brookings, SD 57007, USA
Zhong Hu*
Affiliation:
Department of Mechanical Engineering, South Dakota State University, Brookings, SD 57007, USA
*
a) Address all correspondence to this author. e-mail: zhong.hu@sdstate.edu

Abstract

Nanoindentation techniques are commonly used to characterize nanomechanical properties of microscaled and nanoscaled materials. Nanoindentation using a cylindrical flat-tip indenter has a constant contact area which makes it a reliable source to find material’s yield strength as well as other mechanical properties. However, an angular misalignment of the indenter with the specimen results in experimental error. In this work, the effects of angular misalignment on the nanoindentation testing with a cylindrical flat-tip indenter were numerically analyzed. A three-dimensional nanoindentation solid model was generated, computer modeling based on finite element analysis was conducted. The angle of misalignment ranged from 0° to 1°. Young’s modulus and hardness were evaluated. Based on the hemispherical stress–strain distribution assumption of an elastic plastic indentation, corrected depths and modifiers were proposed for adjusting material’s 0.1% offset and 0.2% offset yield strengths. Low carbon steel AISI 1018 was selected as sample material for indentation testing and modeling validation.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2016 
Figure 0

FIG. 1.Schematic of angular misalignment in nanoindentation using a cylindrical flat-tip indenter.

Figure 1

FIG. 2.3D view of meshed nanoindentation model.

Figure 2

TABLE I.Number of elements and nodes used in modeling.

Figure 3

FIG. 3.Load versus depth for various angular misalignment at maximum depth of 0.35 μm.

Figure 4

TABLE II.Nanoindentation data analysis for different misalignment angles and at various maximum depths (θ = 0°, 0.25°, 0.5°, 0.75°, and 1°, hmax = 0.3, 0.35, and 0.4 μm).

Figure 5

FIG. 4.Hardness versus revised maximum depth for various misalignment angle (θ = 0°, 0.25°, 0.5°, 0.75°, and 1°).

Figure 6

FIG. 5.von Mises stress development in the beginning of the indentation process for different angular misalignments (θ = 0°, 0.25°, and 1°).

Figure 7

FIG. 6.von Mises strain development in the beginning of the indentation process for different angular misalignments (θ = 0°, 0.25°, and 1°).

Figure 8

FIG. 7.Indentation load versus depth comparison for a perfectly elastic and elastoplastic material model at the beginning state for measuring yield strength.

Figure 9

TABLE III.Indentation modeling data for extracting yield strength.

Figure 10

FIG. 8.Misalignment angle versus ratio of depth to radius h′/a or modifier coefficient k.

Figure 11

FIG. 9.Selected profile lines from specimen surface for surface measurement.

Figure 12

FIG. 10.Profile measurement from a typical indentation for estimating angular misalignment: (a) horizontal and (b) vertical.

Figure 13

TABLE IV.Calculated maximum misalignment angles from the indentation profile measurements.

Figure 14

TABLE V.0.1% and 0.2% offset yield strength estimation by indentation testing data.