Hostname: page-component-7b7567c8c-7pwfn Total loading time: 0 Render date: 2026-11-16T18:13:55.680Z Has data issue: false hasContentIssue false

Estimation of Interdiffusivities of the Pseudo NiAl Binary Phase Formed in a Nickel-based Superalloy by Pack Cementation

Published online by Cambridge University Press:  03 March 2011

H. Wei*
Affiliation:
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, The Chinese Academy of Sciences, Shenyang 110016, People’s Republic of China
X.F. Sun
Affiliation:
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, The Chinese Academy of Sciences, Shenyang 110016, People’s Republic of China
Q. Zheng
Affiliation:
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, The Chinese Academy of Sciences, Shenyang 110016, People’s Republic of China
H.R. Guan
Affiliation:
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, The Chinese Academy of Sciences, Shenyang 110016, People’s Republic of China
Z.Q. Hu
Affiliation:
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, The Chinese Academy of Sciences, Shenyang 110016, People’s Republic of China
G.C. Hou
Affiliation:
State Key Laboratory for Corrosion and Protection, Institute of Metal Research, The Chinese Academy of Sciences, Shenyang 110016, People’s Republic of China
*
a) Address all correspondence to this author. e-mail: hwei@imr.ac.cn
Get access

Abstract

The pseudo NiAl binary phase was formed in a nickel-based superalloy by pack cementation. Scanning electron microscopy, transmission electron microscopy, x-ray diffraction, electron probe microanalysis, and positron annihilation technique were used to characterize the pseudo NiAl binary phase. Based on reasonable assumptions, the chemical interdiffusivities of the pseudo NiAl binary phase were then assessed by means of the modified Wagner’s method. The results showed that the chemical interdiffusivities of the pseudo NiAl binary phase were about two orders of magnitude lower than those reported by others. The analysis indicated that the change in thermodynamic properties due to the additions of the microalloying atoms originally present in a superalloy could be responsible mainly for a decrease in chemical interdiffusivities.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable