Hot deformation behaviors of a new hot isostatically pressed nickel based powder metallurgy superalloy

Published online by Cambridge University Press:  03 November 2016

Guoai He
Affiliation:
State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China; Powder Metallurgy Research Institute, Central South University, Changsha 410083, China; and High Temperature Materials Research Institute, Central South University, Changsha 410083, China
Feng Liu
Affiliation:
State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China; Powder Metallurgy Research Institute, Central South University, Changsha 410083, China; and High Temperature Materials Research Institute, Central South University, Changsha 410083, China
Lan Huang*
Affiliation:
State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China; Powder Metallurgy Research Institute, Central South University, Changsha 410083, China; and High Temperature Materials Research Institute, Central South University, Changsha 410083, China
Liang Jiang
Affiliation:
State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China; Powder Metallurgy Research Institute, Central South University, Changsha 410083, China; and High Temperature Materials Research Institute, Central South University, Changsha 410083, China
*
a) Address all correspondence to this author. e-mail: lhuang@csu.edu.cn

Abstract

Hot compression tests of a hot isostatically pressed (HIPed) Ni based powder metallurgy (P/M) superalloy were carried out under various combinations of temperatures and strain rates. To bridge the relationship between stresses and strain rates, constitutive equations were established based on a hyperbolic sine Arrhenius equation, which yielded predicted stresses under the test conditions. It was found that the predict values fit the experimental values with good accuracy. Processing maps of the alloy under the test conditions were established; and the corresponding microstructures after test were examined to elaborate the workability of the alloy. It revealed that surface cracks occurred when strain was higher than 0.25, which initiated at the prior powder boundaries (PPBs) and propagated along the boundaries. The optimum hot working parameters for the alloy were proposed to beat the strain rate of 0.014 s−1 and 1075 °C.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2016 
Figure 0

FIG. 1.Schematic diagram showing (a) the position where the specimens are cut and (b) the dimension of the specimen used for compression.

Figure 1

FIG. 2.Microstructure of as-HIPed Ni based P/M superalloys obtained by SEM.

Figure 2

FIG. 3.Distribution of elements around the PPB of the alloy showing the enrichment of elements: (a) represents the micrograph of as-HIPed alloy, (b)–(n) indicate the distribution of elements of Al, B, C, Co, Cr, Mo, Nb, Ni, O, Ti, W, Zr, Hf, respectively.

Figure 3

FIG. 4.Typical flow stress–strain curves of Ni based superalloy PM-0002 deformed at (a) 0.01 s−1; (b) 0.1 s−1; (c) 1.0 s−1, (d) orientation map obtained by EBSD.

Figure 4

FIG. 5.Relationships between (a) ln σp and $\ln \dot \varepsilon$; (b) σp and $\ln \dot \varepsilon$; (c) ln[sinh(ασp)] and $\ln \dot \varepsilon$; (d) ln[sinh(ασp)] and (1000/T).

Figure 5

TABLE I.Values of n′, β, and α obtained at each temperature and the mean values of these parameters.

Figure 6

FIG. 6.Relationship between ln Z and ln[sinh(ασp)].

Figure 7

FIG. 7.True stress–true strain curves obtained by experiment and predicted values for the alloy at: (a) 1.0 s−1; (b) 0.1 s−1; (c) 0.01 s−1; the predicted values of true stress fits well with the experimental results.

Figure 8

FIG. 8.The correlations between the experimental and predicted flow stress.

Figure 9

FIG. 9.Processing maps of the alloy at different strains: (a) 0.1; (b) 0.2; (c) 0.3; (d) 0.4; (e) 0.5; (f) 0.6; (g) 0.7.

Figure 10

FIG. 10.Microstructure of specimen that deformed to a strain of 0.7 within the instability domain, under conditions of 1025 °C/1.0 s−1.

Figure 11

FIG. 11.EBSD observation of microstructures for specimens deformed to a total strain of 0.7 at given strain rates and temperatures: (a), (c), (e), (g), and (i) represent the deformation temperature of 1000 °C, 1025 °C, 1050 °C, 1075 °C, and 1100 °C at a strain rate of 0.1 s−1, respectively; (b), (d), (f), (h), and (j) represent the deformation temperature of 1000 °C, 1025 °C, 1050 °C, 1075 °C, and 1100 °C at a strain rate of 0.01 s−1, respectively.

Figure 12

FIG. 12.SEM photographs showing the initiation and propagation of cracks deformed at 1075 °C/0.01 s−1: (a) four different periods of cracks and their propagation directions and (b) cracks propagate along the PPB toward the center of the specimen. (c) Fracture surface of the specimen obtained through SEM; (d) individual powder with about 50 μm in diameter.

Figure 13

FIG. 13.Specimen deformed to different strains at optimum hot working conditions of 1075 °C/0.01 s−1: (a) macro-profile; (b) microstructure of specimen at a strain of 0.25; (c) distribution of grain size.