Indium-tin oxide thin films by metal-organic decomposition

Published online by Cambridge University Press:  03 March 2011

Dennis Gallagher
Affiliation:
Laboratoire de Technologie des Poudres, École Polytechnique Fédérale de Lausanne, CH-1015 Lausanne, Switzerland
Francis Scanlan
Affiliation:
Laboratoire de Technologie des Poudres, École Polytechnique Fédérale de Lausanne, CH-1015 Lausanne, Switzerland
Raymond Houriet
Affiliation:
Laboratoire de Technologie des Poudres, École Polytechnique Fédérale de Lausanne, CH-1015 Lausanne, Switzerland
Hans Jörg Mathieu
Affiliation:
Laboratoire de Technologie des Poudres, École Polytechnique Fédérale de Lausanne, CH-1015 Lausanne, Switzerland
Terry A. Ring*
Affiliation:
Laboratoire de Technologie des Poudres, École Polytechnique Fédérale de Lausanne, CH-1015 Lausanne, Switzerland
*
d)Author to whom correspondence should be sent.
Get access

Abstract

In2O3–SnO2 films were produced by thermal decomposition of a deposit which was dip coated on borosilicate glass substrates from an acetylacetone solution of indium and tin acetoacetonate. Thermal analysis showed complete pyrolysis of the organics by 400 °C. The thermal decomposition reaction generated acetylacetone gas and was found to be first order with an activation energy of 13.6 Kcal/mole. Differences in thermal decomposition between the film and bulk materials were noted. As measured by differential scanning calorimetry using a 40 °C/min temperature ramp, the glass transition temperature of the deposited oxide film was found to be ∼462 °C, and the film crystallization temperature was found to be ∼518 °C. For film fabrication, thermal decomposition of the films was performed at 500 °C in air for 1 h followed by reduction for various times at 500 °C in a reducing atmosphere. Crystalline films resulted for these conditions. A resistivity of ∼1.01 × 10−3 Ω · cm, at 8 wt. % tin oxide with a transparency of ∼95% at 400 nm, has been achieved for a 273 nm thick film.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 1993

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable