Hostname: page-component-7b7567c8c-7pwfn Total loading time: 0 Render date: 2026-11-16T21:48:44.185Z Has data issue: false hasContentIssue false

Intermetal dielectric process using spin-on glass for ferroelectric memory devices having SrBi2Ta2O9 capacitors

Published online by Cambridge University Press:  31 January 2011

Suk-Kyoung Hong*
Affiliation:
FeRAM Technology, Memory R–1, Ami-ri, Bubal-eub, Ichon-si, Kyoungki-do, 467–701 Korea
Yang Han Yoon
Affiliation:
Process Development Thin-Film, Memory R–1, Ami-ri, Bubal-eub, Ichon-si, Kyoungki-do, 467–701 Korea
Yong Ku Baek
Affiliation:
FeRAM Technology, Memory R–1, Ami-ri, Bubal-eub, Ichon-si, Kyoungki-do, 467–701 Korea
Chang Goo Lee
Affiliation:
FeRAM Technology, Memory R–1, Ami-ri, Bubal-eub, Ichon-si, Kyoungki-do, 467–701 Korea
Chung Won Suh
Affiliation:
FeRAM Technology, Memory R–1, Ami-ri, Bubal-eub, Ichon-si, Kyoungki-do, 467–701 Korea
Seok Won Lee
Affiliation:
FeRAM Technology, Memory R–1, Ami-ri, Bubal-eub, Ichon-si, Kyoungki-do, 467–701 Korea
Young Min Kang
Affiliation:
FeRAM Technology, Memory R–1, Ami-ri, Bubal-eub, Ichon-si, Kyoungki-do, 467–701 Korea
Nam Soo Kang
Affiliation:
FeRAM Technology, Memory R–1, Ami-ri, Bubal-eub, Ichon-si, Kyoungki-do, 467–701 Korea
Cheol Seong Hwang*
Affiliation:
School of Material Science and Engineering, Seoul National University, San #56–1 Shillim-dong, Kwanak-ku, Seoul, 151–742, Korea
Oh Seong Kwon
Affiliation:
School of Material Science and Engineering, Seoul National University, San #56–1 Shillim-dong, Kwanak-ku, Seoul, 151–742, Korea
Get access

Abstract

The degradation behavior of integrated Pt/SrBi2Ta2O9/Pt capacitors caused by hydrogen impregnation during the spin-on glass (SOG)-based intermetal dielectric (IMD) process was investigated. SOG was tested as an IMD since it offers better planarity for multilevel metallization processes compared to other SiO2 deposition methods. It was found that the SOG itself does not degrade the ferroelectric performance. Deposition of an under-layer of SiOxNy by plasma-enhanced chemical vapor deposition (PECVD) using SiH4 + N2O + N2 source gases and a SiO2?x capping layer by another PECVD process using SiH4 + N2O source gases produced hydrogen as a reaction by-product. The hydrogen diffused into the SBT layer and degraded the ferroelectric performance during subsequent annealing cycles. A very thin (10 nm) Al2O3 layer grown by atomic layer deposition before the IMD process successfully blocked the impregnation of the hydrogen. Therefore, excellent ferroelectric performance of the SBT capacitors were maintained after the multilevel metallization process as well as passivation. The adoption of SOG in the IMD process greatly improved the surface flatness of the wafer resulting in a higher capacitor yield with very good uniformity in ferroelectric properties over the 8-in.-diameter wafer.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2000

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable