Irreversible hydrogenation of solid C60 with and without catalytic metals

Published online by Cambridge University Press:  31 January 2011

Eric L. Brosha
Affiliation:
Los Alamos National Laboratory, Los Alamos, New Mexico 87545
John Davey
Affiliation:
Los Alamos National Laboratory, Los Alamos, New Mexico 87545
Fernando H. Garzon
Affiliation:
Los Alamos National Laboratory, Los Alamos, New Mexico 87545
Shimshon Gottesfeld
Affiliation:
Los Alamos National Laboratory, Los Alamos, New Mexico 87545
Get access

Abstract

The dehydrogenation of C60 · H18.7 was studied using thermogravimetric and powder x-ray diffraction analysis. C60 · H18.7 was found to be stable up to 430 °C in Ar at which point the release of hydrogen initiated the collapse of a fraction of fullerene molecules. X-ray diffraction analysis performed on C60 · H18.7 samples dehydrogenated at 454, 475, and 600 °C displayed an increasing volume fraction of amorphous material. The decomposition product comprises randomly oriented, single-layer graphite sheets. Evolved gas analysis using gas chromatograph (GC) mass spectroscopy confirmed the presence of both H2 and methane upon dehydrogenation. Attempts to improve reversibility or reduce hydrogenation/ dehydrogenation temperatures by addition of Ru and Pt catalysts were unsuccessful.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable