Hostname: page-component-7b7567c8c-kwt9d Total loading time: 0 Render date: 2026-11-12T07:20:54.501Z Has data issue: false hasContentIssue false

Modeling nanoindentation using the Material Point Method

Published online by Cambridge University Press:  25 May 2018

Chad C. Hammerquist
Affiliation:
Wood Science and Engineering, Oregon State University, Corvallis, Oregon 97330, USA
John A. Nairn*
Affiliation:
Wood Science and Engineering, Oregon State University, Corvallis, Oregon 97330, USA
*
a)Address all correspondence to this author. e-mail: john.nairn@oregonstate.edu

Abstract

A numerical nanoindentation model was developed using the Material Point Method (MPM), which was chosen because it can handle both large deformations and dynamic contact under the indenter. Because of the importance of contact, prior MPM contact methods were enhanced to improve their accuracy for contact detection. Axisymmetric and full 3D simulations investigated the effects of hardening, strain-rate dependent yield properties, and local structure under the indenter. Convergence of load–displacement curves required small cells under the indenter. To reduce computation time, we used an effective nonregular grid, called a tartan grid and describe its implementation. Tartan grids reduced simulation times by an order of magnitude. A series of simulated load–displacement curves were analyzed as “virtual experiments” by standard Oliver–Pharr methods to extract effective modulus and hardness of the indented material. We found that standard analysis methods give results that are affected by hardening parameters and strain-rate dependence of plasticity. Because these parameters are not known during experiments, extracted properties will always have limited accuracy. We describe an approach for extracting more properties and more accurate properties by combining MPM simulations with inverse methods to fit simulation results to entire load–displacement curves.

Information

Type
Article
Copyright
Copyright © Materials Research Society 2018 
Figure 0

FIG. 1.Axisymmetric MPM simulation of nanoindentation with colors (or shades of gray) showing radial displacement. (a) The full modeled specimen from an axisymmetric simulation. (b) Zoomed-in view of the absolute value of transverse displacements from a 3D simulation using a Berkovich indenter.

Figure 1

FIG. 2.(a) Cross plot of load output versus displacement input for typical simulated indenter load as a function of displacement for both loading and unloading. (b) Simulated load–displacement curves for a strain-rate dependent material with Cjc = 0.1 for different hold times.

Figure 2

FIG. 3.The percent error in effective modulus extrapolated from simulated nanoindentation curves as a function of the percentage of the unloading curves used in the analysis. The three curves are for three methods for choosing ε in the analysis method. All curves used β = 1.05.

Figure 3

FIG. 4.Effect of scaling the hardening parameters on parameters extracted from load–displacement curves. (a) Percent error in calculated effective modulus. (b) Calculated hardness. All curves used ε = 0.75 and β = 1.115.

Figure 4

FIG. 5.Effect of Cjc and hold times on parameters extracted from load–displacement curves. (a) Calculated hardness. (b) Percent error in calculated effective modulus. All curves used ε = 0.75 and β = 1.115.

Figure 5

FIG. 6.Axisymmetric simulation geometries used to investigate the effect of structure on shape. d is the distance from indentation tip to a key structural change. A—Low stiffness material surrounded by high stiffness material (moduli in GPa). B—High stiffness material surrounded by low stiffness. C—Thin material.

Figure 6

FIG. 7.The effect of distance to a structural change on effective modulus extracted from simulated nanoindentation curves. The horizontal dashed lines are the actual effective moduli. Plots a and b show the same date plotted in two different ways.

Figure 7

FIG. 8.Comparison of the actual indenter shapes, effective indenter shapes, and an isosurface of vertical compressive stress of 30 MPa under the indenter. The vertical axis for the shapes was made five times larger and all the geometries are flipped upside down, and the flat surface was added for better viewing perspective.

Supplementary material: PDF

Hammerquist and Nairn supplementary material

Hammerquist and Nairn supplementary material

Download Hammerquist and Nairn supplementary material(PDF)