Nanoindentation investigations to study solid solution hardening in Ni-based diffusion couples

Published online by Cambridge University Press:  31 January 2011

Oliver Franke
Affiliation:
Department for Materials Science, Institute I, General Materials Properties, University Erlangen-Nürnberg, Erlangen D-91508, Germany
Karsten Durst*
Affiliation:
Department for Materials Science, Institute I, General Materials Properties, University Erlangen-Nürnberg, Erlangen D-91508, Germany
Mathias Göken
Affiliation:
Department for Materials Science, Institute I, General Materials Properties, University Erlangen-Nürnberg, Erlangen D-91508, Germany
*
a) Address all correspondence to this author. e-mail: karsten.durst@ww.uni-erlangen.de
Get access

Abstract

In this work the hardening effect of Ta and Mo in Ni-base alloys was investigated using a combinatorial approach with diffusion couples. Furthermore, the Ni-Fe system was used as a reference system taking advantage of the full miscibility at high temperatures. Ta was chosen, as aside from having a technical relevance in the Ni-base superalloys, it also has a high miscibility in Ni. The main focus of this paper will be solid solution hardening. It will be shown that even though the determination of hardness is subject to varying indentation size effects (ISE) [Durst et al., Acta Mater.55(20), 6825 (2007)], only a few modifications are necessary to describe solid solution strengthening measured by nanoindentations using the Labusch theory [Labusch, Acta Metall.20(7), 917 (1972)]. Moreover, after a careful evaluation of the results, the data can be used to investigate solid solution hardening effects quickly and efficiently with small amounts of material.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable