Preparation of Colloidal Bismuth Particles in Polyols

Published online by Cambridge University Press:  01 June 2005

Corina Goia
Affiliation:
Center for Advanced Materials Processing, Clarkson University, Potsdam, New York 13699-5814
Egon Matijević
Affiliation:
Center for Advanced Materials Processing, Clarkson University, Potsdam, New York 13699-5814
Dan V. Goia
Affiliation:
Center for Advanced Materials Processing, Clarkson University, Potsdam, New York 13699-5814
Get access

Abstract

Nano- and micrometer size spherical bismuth particles were prepared by reducing bismuth salts in simple and mixed polyols at elevated temperatures. In general, the conversion to metallic bismuth was preceded by the formation, at intermediate temperatures, of bismuth-polyol compounds. By changing the type of bismuth salt, the composition of the polyol mixture, and the temperature of the process, these precursors were successfully converted into spherical bismuth particles. It was found that the reduction process proceeds only if the temperature of the polyol exceeds the values at which the intermediate bismuth-polyol are stable, which was determined to be around 220 °C.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable