Abstract

The solid-phase epitaxy of LiNbO3 following ion implantation of Ti dopant for the purpose of producing optical waveguides has been studied. Implanting 360-keV Ti at liquid nitrogen temperature produces a highly damaged region extending to a depth of about 400 nm. This essentially amorphous region can be recrystallized epitaxially by annealing in a water-saturated oxygen atmosphere at temperatures near 400 °C. though complete removal of all irradiation-induced damage requires temperatures in excess of 600 °C. The activation energy of the regrowth is 2.0 eV for implanted fluences below 3 ⊠ 1016 Ti/cm2. At higher fluences the regrowth proceeds more slowly, and Ti dopant segregates at the regrowth interface. Complete recrystallization following high-dose implantation requires annealing temperatures in excess of 800 °C.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 1989

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable