Synthesis and pressureless sintering of Ti3SiC2 powder

Published online by Cambridge University Press:  31 January 2011

Seong-Jai Cho*
Affiliation:
Division of Advanced Technology, Korea Research Institute of Standards and Science, Yuseong, Daejeon, 305-340, Republic of Korea
*
b) Address all correspondence to these authors. e-mail: sjcho@kriss.re.kr
Get access

Abstract

Ti3SiC2 powder of about 96 wt% purity was produced using TiCx and Si powders. The synthesis process was characterized by an exothermic reaction at ∼985 °C and low activation energy (∼27 kJ/mol) of conversion. Almost complete conversion to Ti3SiC2 phase was observed during sintering. The onset temperature of sintering was found to be at about 1060 °C using dilatometer. The density of nearly 99% (theoretical) was achieved through the pressureless sintering of Ti3SiC2 powder by 1 and 2 wt% Si powder additions. The sample (without sintering aid) sintered at 1500 °C for 4 h showed uniformly distributed angular grains, whereas the bimodal nature of the microstructure was observed when Si was added as a sintering aid.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable