Hostname: page-component-7b7567c8c-7pwfn Total loading time: 0 Render date: 2026-11-17T10:46:01.857Z Has data issue: false hasContentIssue false

Synthesis of YBa2Cu3O7−δ with clean grain boundaries by a modified aerosol decomposition process

Published online by Cambridge University Press:  31 January 2011

Yuan-Liang Wang
Affiliation:
Materials Science Division, Brookhaven National Laboratory, Upton, New York 11973-5000
Z.Q. Tan
Affiliation:
Materials Science Division, Brookhaven National Laboratory, Upton, New York 11973-5000
Yimei Zhu
Affiliation:
Materials Science Division, Brookhaven National Laboratory, Upton, New York 11973-5000
A.R. Moodenbaugh
Affiliation:
Materials Science Division, Brookhaven National Laboratory, Upton, New York 11973-5000
M. Suenaga
Affiliation:
Materials Science Division, Brookhaven National Laboratory, Upton, New York 11973-5000
Get access

Abstract

A modified aerosol decomposition method was developed for producing sintered YBa2Cu3O7−δ (1-2-3) pellets having sharp superconducting transition Tc's at ∼90 K, fine grain sizes, and clean grain boundaries. This method used “precursor” powders, which were produced with an aerosol flow reactor at 550 °C, instead of in situ produced 1-2-3 powders commonly processed at 880–1000 °C. As determined by x-ray absorption and powder diffraction studies, the 1-2-3 powders produced by the modified route contain less cation disorders than the in situ produced powders. The disorder is speculated to be the cause of Tc-suppression and broadening. It cannot be removed unless high sintering temperatures were used (>950 °C), which resulted in large grains and impurities and cracks at grain boundaries.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable