Hostname: page-component-7b7567c8c-8tzhz Total loading time: 0 Render date: 2026-11-19T17:04:48.746Z Has data issue: false hasContentIssue false

Zr-Cu-Ni-Al-Ta glassy matrix composites with enhanced plasticity

Published online by Cambridge University Press:  01 June 2006

Wenbo Dong
Affiliation:
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
Haifeng Zhang*
Affiliation:
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
Wensheng Sun
Affiliation:
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
Aimin Wang
Affiliation:
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
Hong Li
Affiliation:
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
Zhuangqi Hu
Affiliation:
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
*
a) Address all correspondence to this author. e-mail: hfzhang@imr.ac.cn
Get access

Abstract

(Zr62Cu15.4Ni12.6) (x = 6–12) in situ glassy composites containing uniformly distributed Ta-rich particles were prepared by arc-melting and copper mould casting. The results show that addition of 6–10 at.% Ta to Zr62Cu15.4Ni12.6Al10 results in dissolution of 2.4 to 4.6 at.% Ta in the glassy matrix, which promotes glass-forming ability, and the remaining Ta precipitates out as body-centered cubic (BCC) Ta-rich particles dispersed on the glassy matrix. The critical diameters for the composites with 6, 8, and 10 at.% Ta are 7, 7, and 6 mm, respectively. At 12 at.% Ta addition, the glass-forming ability is dramatically reduced because of the precipitation of secondary dendritic Ta-rich particles and other nanocrystallites from melts during copper mould casting. Also, owing to the solid-liquid reaction during induction heating, some Ta-rich particles formed in the master alloys will redissolve into the glassy matrix, resulting in a smaller volume fraction of Ta-rich particles in the as-cast glassy rods than that of the corresponding ingots. The glassy matrix composites exhibit enhanced plastic strain of about 7.5 to 22.5% at room temperature. The optimum Ta content in the glassy alloys is determined to be 10 at.%, which corresponds to the highest ultimate stress of 2220 MPa and the largest plastic strain of 22.5%. The plastic strain increases with increasing volume fraction of in situ BCC Ta-rich particles. This is apparently ascribed to the impedance of Ta-rich particles to shear bands. Ta-rich particles seed the initiation of multiple shear bands and block the shear band propagation, leading to intensive multiplication and bifurcation of shear bands.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2006

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable