Hostname: page-component-7b7567c8c-wxvwp Total loading time: 0 Render date: 2026-11-16T23:14:57.711Z Has data issue: false hasContentIssue false

Electrical Characterization and Nanoindentation of Opto-electro-mechanical Percolative Composites from 2D Layered Materials

Published online by Cambridge University Press:  03 August 2017

Jorge A. Catalán
Affiliation:
Department of Metallurgical, Materials and Biomedical Engineering, University of Texas at El Paso, El Paso, TX 79968, U.S.A.
Ricardo Martínez
Affiliation:
Department of Mechanical Engineering, University of Texas at El Paso, El Paso, TX 79968, U.S.A.
Yirong Lin
Affiliation:
Department of Mechanical Engineering, University of Texas at El Paso, El Paso, TX 79968, U.S.A.
Anupama B. Kaul*
Affiliation:
Department of Electrical and Computer Engineering, University of Texas at El Paso, El Paso, TX 79968, U.S.A.
*
*E-mail: akaul@utep.edu
Get access

Abstract

In this paper, we have developed composites with Poly-methyl methacrylate (PMMA) as the matrix material, while transition metal dichalcogenides (TMDCs), MoS2 and WS2 and graphite served as the filler materials. The PMMA was chosen as the matrix material due to its low-cost, wide availability, as well as its promising mechanical and optical properties for enabling opto-electro-mechanical sensing devices. The amount of filler material used ranged from 100 mg/ml up to 400 mg/ml. With the aid of designed fixtures we related the electrical properties of the PMMA-based composite sensors to the degree of strain or deformation. Additionally, a nanoindenter was used to measure the modulus of elasticity, with values as low as 2 GPa and as high as 20 GPa for the graphite composites, and hardness values which ranged from 0.1 GPa to ∼ 1.6 GPa.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2017 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable