Hostname: page-component-7b7567c8c-fvjsw Total loading time: 0 Render date: 2026-11-16T16:33:05.850Z Has data issue: false hasContentIssue false

Diamond Schottky Barrier Diode with Fluorine- andOxygen-Termination

Published online by Cambridge University Press:  15 February 2016

Chao Hu
Affiliation:
Institute of wide band gap semiconductors, Xi'an Jiaotong University, Xi'an, China.
Zhangcheng Liu
Affiliation:
Institute of wide band gap semiconductors, Xi'an Jiaotong University, Xi'an, China.
Jingwen Zhang
Affiliation:
Institute of wide band gap semiconductors, Xi'an Jiaotong University, Xi'an, China.
Wei Wang
Affiliation:
Institute of wide band gap semiconductors, Xi'an Jiaotong University, Xi'an, China.
Hong-Xing Wang*
Affiliation:
Institute of wide band gap semiconductors, Xi'an Jiaotong University, Xi'an, China.
Get access

Abstract

Schottky properties of Mo on diamond with fluorine- and oxygen-termination hadbeen investigated. Oxygen-termination was generated by aqua regia.Fluorine-termination was generated by CF4 plasma treatment. Mo/Ni/Auwas deposited on the diamond surface as Schottky electrode, whose barrier heightwas evaluated from current-voltage curve. After that, the X-ray photoelectronspectroscopy methods were applied to calculate the Schottky barrier height of Moon different termination surface. The results indicated that thefluorine-termination and oxygen-termination show different schottkyproperties.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2016 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable