Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-17T13:25:55.261Z Has data issue: false hasContentIssue false

A New Nanoindentation Protocol for Identifying the Elasticity ofUndamaged Extracellular Bone Tissue

Published online by Cambridge University Press:  15 February 2016

Irina Furin
Affiliation:
Institute for Mechanics of Materials and Structures, TU Wien - Vienna University of Technology, Austria
Maria-Ioana Pastrama
Affiliation:
Institute for Mechanics of Materials and Structures, TU Wien - Vienna University of Technology, Austria
Hawraa Kariem
Affiliation:
Institute for Mechanics of Materials and Structures, TU Wien - Vienna University of Technology, Austria
Krzysztof W. Luczynski
Affiliation:
Institute for Mechanics of Materials and Structures, TU Wien - Vienna University of Technology, Austria
Olaf Lahayne
Affiliation:
Institute for Mechanics of Materials and Structures, TU Wien - Vienna University of Technology, Austria
Christian Hellmich*
Affiliation:
Institute for Mechanics of Materials and Structures, TU Wien - Vienna University of Technology, Austria
*
1Corresponding author E-mail address: christian.hellmich@tuwien.ac.at (Christian Hellmich)
Get access

Abstract

While the quest for understanding and even mimicking biological tissue haspropelled, over the last decades, more and more experimental activities at themicro and nanoscales, the appropriate evaluation and interpretation ofrespective test results has remained a formidable challenge. As a contributionto tackling this challenge, we here describe a new method for identifying, fromnanoindentation, the elasticity of the undamaged extracellular bone matrix. Theunderlying premise is that the tested bovine bone sample is either initiallydamaged (i.e. exhibits micro-cracks a priori) or that suchmicro-cracks are actually induced by the nanoindentation process itself, orboth. Then, (very many) indentations may relate to either an intact materialphase (which is located sufficiently far away from micro-cracks), or todifferently strongly damaged material phases. Corresponding elastic phaseproperties are identified from the statistical evaluation of the measuredindentation moduli, through representation of their histogram as a weighted sumof Gaussian distribution functions. The resulting undamaged elastic modulus ofbovine femoral extracellular bone matrix amounts to 31 GPa, a value agreeingstrikingly well both with direct quasi-static modulus tests performed onSEM-FIB-produced micro-pillars (Luczynski et al., 2015), and with thepredictions of a widely validated micromechanics model (Morin and Hellmich,2014). Further confidence is gained through observing typical indentationimprints under Scanning Electron Microscopy (SEM), which actually confirms theexistence of the two types of micro-cracks as described above.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2016 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable