Hostname: page-component-7b7567c8c-8tzhz Total loading time: 0 Render date: 2026-11-19T20:17:34.835Z Has data issue: false hasContentIssue false

Synthesis and characterization of polypyrrole thin films in a resistive plasma reactor by high frequency

Published online by Cambridge University Press:  24 January 2020

E. De la Cruz-Reyes*
Affiliation:
Tecnologico Nacional de México/Instituto Tecnológico de Toluca, Av. Tecnológico s/n. Agrícola Bella Vista C.P.52149 Metepec, Edo. De México, México.
C. Hernández-Tenorio
Affiliation:
Tecnologico Nacional de México/Instituto Tecnológico de Toluca, Av. Tecnológico s/n. Agrícola Bella Vista C.P.52149 Metepec, Edo. De México, México.
M. Villanueva-Castañeda
Affiliation:
Tecnologico Nacional de México/Instituto Tecnológico de Toluca, Av. Tecnológico s/n. Agrícola Bella Vista C.P.52149 Metepec, Edo. De México, México.
H. Moreno-Saavedra
Affiliation:
Tecnologico Nacional de México/Instituto Tecnológico de Toluca, Av. Tecnológico s/n. Agrícola Bella Vista C.P.52149 Metepec, Edo. De México, México.
R. Alejo-Eleuterio
Affiliation:
Tecnologico Nacional de México/Instituto Tecnológico de Toluca, Av. Tecnológico s/n. Agrícola Bella Vista C.P.52149 Metepec, Edo. De México, México.
Get access

Abstract

Polypyrrole (PPy) thin films were synthetized by plasma and simultaneously doped with Iodine to enhance electromagnetic absorption and charge transfer capability in a resistive coupling cylindrical reactor. Pyrrole monomer and Iodine were the principal reagents used and the chemical reactions were created by high frequency plasma. Micrographs show an irregular surface formed by semi-spherical protrusions with tiny particles in the PPy/I samples and a rather smooth surface with wrinkles and less participation of tiny particles to PPy ones. Infrared spectroscopy analysis reveals important absorption peaks at 3253, 2932, 1668 and 635 cm-1 corresponding to the chemical bonds N-H and C-H, C-H aliphatic, C=C and C-I, respectively, belonging to the chemical structure of Pyrrole. Electrical conductivity of PPy increased from 10-10 to 10-8 S/cm due to Iodine doping. Electromagnetic absorption showed a higher response between 340 and 800 nm in the visible region. Activation energy was calculated in the range from -0.09 to 0.49 eV.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2020 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable