The Dynamics of Deposit Formation in Thermal-Spray Processes

Published online by Cambridge University Press:  31 January 2011

Get access

Extract

In thermal spraying, coatings are formed by particles flattening and piling up on the substrate. At impact, the sudden deceleration of the particle causes a pressure buildup at the particle-surface interface; the high pressure inside the particle forces melted material to flow laterally and ductile material to deform. The particle spreads outward from the point of impact and forms a “splat.” The arresting of spreading results from the conversion of particle kinetic energy into work of viscous deformation and surface energy. Solidification constraint (when the solidification front is advancing from the substrate surface fast enough to interact with the liquid during spreading) and mechanical constraint (due to the roughness of the substrate surface) can interfere with the flattening process.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2000

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable