Hostname: page-component-7b7567c8c-kwt9d Total loading time: 0 Render date: 2026-11-12T16:34:08.884Z Has data issue: false hasContentIssue false

Novel materials by atomic layer deposition and molecular layer deposition

Published online by Cambridge University Press:  18 November 2011

Markku Leskelä
Affiliation:
University of Helsinki, Finland; markku.leskela@helsinki.fi
Mikko Ritala
Affiliation:
University of Helsinki, Finland; Mikko.Ritala@helsinki.fi
Ola Nilsen
Affiliation:
University of Oslo, Norway; ola.nilsen@kjemi.uio.no

Abstract

Over the past 10 years, the number of materials that can be processed by atomic layer deposition (ALD) has expanded rapidly. Significant progress has been seen in ALD of high-κ oxides, ternary oxides, and noble metals, which have been studied quite extensively. High-κ oxide processes are used today in various industrial applications. However, many new applications are pushing the need for less common compounds, and therefore new processes are being developed (e.g., for fluorides, Li containing compounds, and phosphates). New ALD processes require new designs for volatile precursors to deliver elements with ligands that ensure self-limiting surface reactions. In addition to inorganics, new polymeric and inorganic-organic hybrid materials are opening new frontiers for ALD, including expansion of the process to include molecular layer deposition. A combination of inorganic and organic parts in the deposited layers offers expanding opportunities for tailoring materials properties.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2011
Figure 0

Figure 1.Leak current density at 0.8 V versus capacitance equivalent thickness (tox) for TiO2 and TiO2:Al films with different cycle ratios (1:60, 1:90, 1:120). The dashed line shows the acceptable leakage current level (10–7 A/cm2).8 ATO, aluminum-doped TiO2. Reprinted with permission. © 2008, Wiley.

Figure 1

Figure 2.Cross-sectional scanning election microscopy images of a ZrO2 film grown by the CpZr(NMe2)3/O3 process at 275°C into 60:1 aspect ratio trenches. The upper image shows the top part of the trench, and those below are the middle and bottom parts. The trench opening is 115 nm wide with a depth of 6.75 mm. Labels denote the ZrO2 film thicknesses.11 Cp = cyclopentadienyl; Me = methyl. Reprinted with permission. © 2008, Royal Chemical Society.

Figure 2

Figure 3.Quartz crystal microbalance data measured during the reaction cycles for RuCp2 and O2. m0 denotes the total mass change during one complete reaction cycle, and m1 denotes the mass change during the RuCp2 pulse. Note that the mass increases during the O2 pulse and decreases during RuCp2 pulse, indicating adsorption of excess oxygen onto the surface.32 Reprinted with permission. © 2005, Electrochemical Society.

Figure 3

Figure 4.Suggested reaction schemes for CaF2 atomic layer deposition (ALD) during the (a) Ca(thd)2 pulse and (b) TiF4 pulse.39 Note: thd, = 2,2,6,6-tetramethyl-3,5-heptanedione. The incoming Ca(thd)2 reacts with the TiFx terminated surface forming CaF2 on the substrate and Ti(thd)4 vapor. When the Ca(thd)2 dose is high enough, it forms a Ca(thd)x terminated surface. In the next step, the incoming TiF4 reacts with the Ca(thd)x terminated surface and also forms solid CaF2 and Ti(thd)4 vapor. A high TiF4 dose saturates the surface, leaving TiFx surface groups, and the cycle can start again. Reprinted with permission. © 2007, American Chemical Society.

Figure 4

Figure 5.Resistivity (R) versus temperature (T) data for Ge-Sb-Te (GST) films made by atomic layer deposition (ALD) (open boxes) and sputtering (closed boxes) showing very similar behavior.46 Reprinted with permission. © 2009, Elsevier.

Figure 5

Figure 6.Conformability of the SbCl3-(Et3Si)3Sb atomic layer deposition (ALD) process. (a) Cross-section field-emission scanning electron microscope (FESEM) image of a Sb film deposited on a high-aspect-ratio trench structure. (b)–(d) FESEM images of Sb nanotubes prepared using a porous alumina membrane as a template. The deposition temperature was 100°C, and the number of ALD cycles was 1000. Pulse/purge times were 2/10 s for SbCl3 and 4/10 s for (Et3Si)3Sb.47 Et = ethyl. Reprinted with permission. © 2011, American Chemical Society.

Figure 6

Figure 7.Schematic of a three-step (ABC) growth process for the deposition of an organic-inorganic hybrid material using a sequence of (a) trimethylaluminum, (b) ethanolamine, and (c) maleic anhydride, where an imide bond also forms.73 Reprinted with permission. © 2009, American Chemical Society.