Hostname: page-component-7b7567c8c-2n9c9 Total loading time: 0 Render date: 2026-11-17T04:33:02.063Z Has data issue: false hasContentIssue false

Comparison of the Young's moduli of polymers measured from nanoindentation and bending experiments

Published online by Cambridge University Press:  21 July 2014

Ricardo Martinez
Affiliation:
Department of Mechanical Engineering, University of Texas at El Paso, El Paso, Texas 79968
L. Roy Xu*
Affiliation:
Department of Mechanical and Aerospace Engineering, New Mexico State University, Las Cruses, New Mexico 88003
*
Address all correspondence to L. Roy Xu at luoyu.r.xu@gmail.com

Abstract

Spherical and conical nanoindentation experiments were performed for the same polymer specimens to compare Young's moduli measured from the elastic loading and unloading curves, and bending experiments. Finite-element simulation was employed to ensure pure elastic deformation during spherical nanoindentation. The moduli measured from the elastic loading curves using Hertz's contact law are very close to the bending moduli, because both measurements were conducted under the same elastic deformation. However, the moduli measured from the elastic unloading curves are up to 60% higher than the bending moduli owing to plastic deformation close to the sharp conical indenter tip.

Information

Type
Research Letters
Copyright
Copyright © Materials Research Society 2014 
Figure 0

Figure 1.A typical load–displacement curve for a nanoindentation process.

Figure 1

Figure 2.A spherical nanoindentation force/displacement curve showing zero displacement but non-zero indentation force of a PMMA sample.

Figure 2

Table I.Young's moduli of two kinds of polymers using three approaches.

Figure 3

Figure 3.Comparison of a simulated force–indentation depth curve (solid line) and some experimental curves (points) for PC specimens.

Supplementary material: File

Martinez and Xu Supplementary Material

Figures S1-S3

Download Martinez and Xu Supplementary Material(File)