Hostname: page-component-7b7567c8c-fvjsw Total loading time: 0 Render date: 2026-11-17T00:11:02.955Z Has data issue: false hasContentIssue false

Arrayed ZnO Nanorods Fabrication on ZnO Film by Self-catalyst Growth Method in Aqueous Solution

Published online by Cambridge University Press:  02 January 2014

E. K.C. Pradeep
Affiliation:
Institute for Nanotechnology, Kochi University of Technology, Kami city, Kochi 782-8502, JAPAN
X. Li*
Affiliation:
Institute for Nanotechnology, Kochi University of Technology, Kami city, Kochi 782-8502, JAPAN
T. Kawaharamura
Affiliation:
Institute for Nanotechnology, Kochi University of Technology, Kami city, Kochi 782-8502, JAPAN
D. Wang
Affiliation:
Department of Environmental Science and Engineering, Kochi University of Technology, Kami city, Kochi 782-8502, JAPAN
A. Hatta
Affiliation:
Institute for Nanotechnology, Kochi University of Technology, Kami city, Kochi 782-8502, JAPAN
C. Li*
Affiliation:
Institute for Nanotechnology, Kochi University of Technology, Kami city, Kochi 782-8502, JAPAN
Get access

Abstract

ZnO nanorods were grown up from as-deposited ZnO film on which the zinc self-catalysts generated by a novel reducing method. Well aligned ZnO nanorods with a uniform high aspect ratio were grown up on multi-annealed samples. The length of nanorods depended significantly on the reaction time in the hydrothermal synthesis.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable