Hostname: page-component-7b7567c8c-fvjsw Total loading time: 0 Render date: 2026-11-17T17:35:19.770Z Has data issue: false hasContentIssue false

Bone-Bonding Ability of Anodized Titanium Plate Loaded With Hydroxyapatite Particles

Published online by Cambridge University Press:  15 March 2011

Mitsunobu Iwasaki
Affiliation:
Department of Applied Chemistry, School of Science and Engineering, Kinki University, 3-4-1 Kowakae, Higashi-Osaka, Osaka, 577-8502, Japan
Kohki Kudo
Affiliation:
Department of Applied Chemistry, School of Science and Engineering, Kinki University, 3-4-1 Kowakae, Higashi-Osaka, Osaka, 577-8502, Japan
Kazuki Shimada
Affiliation:
Department of Applied Chemistry, School of Science and Engineering, Kinki University, 3-4-1 Kowakae, Higashi-Osaka, Osaka, 577-8502, Japan
Kohji Matsuzaki
Affiliation:
Department of Orthopedic Surgery, School of Medicine, Kinki University, 377-2 Ohno-Higashi, Osaka-Sayama, Osaka 589-8511, Japan
Chiaki Hamanishi
Affiliation:
Department of Orthopedic Surgery, School of Medicine, Kinki University, 377-2 Ohno-Higashi, Osaka-Sayama, Osaka 589-8511, Japan
Get access

Abstract

Submicron-sized hydroxyapatite (HAp) particles were loaded on the titanium plate by anodic oxidation over spark discharge voltage in HAp-containing bath. The biocompatibility and bioactivity were drastically improved by HAp deposition on the anodic oxide films. The affinity with living bone was the following order: anodized titanium plate with HAp > anodized titanium plate ≫ titanium. Bone-bonding strength between HAp-loaded titanium plate and living bone after 4 weeks' implant was much higher than that of anodized titanium plate.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable