Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-18T15:29:07.410Z Has data issue: false hasContentIssue false

Creep in Single Crystal Ni3AI

Published online by Cambridge University Press:  15 February 2011

W. Zhu
Affiliation:
School of Metallurgy and Materials, University of Birmingham, Birmingham B15 2TT, England
I. P. Jones
Affiliation:
School of Metallurgy and Materials, University of Birmingham, Birmingham B15 2TT, EnglandIRC in Materials for High Performance Applications, University of Birmingham, Birmingham B15 2TT, England
D. Fort
Affiliation:
School of Metallurgy and Materials, University of Birmingham, Birmingham B15 2TT, England
R. E. Smallman
Affiliation:
School of Metallurgy and Materials, University of Birmingham, Birmingham B15 2TT, England
Get access

Abstract

Single crystals of Ni3AI (1 at%Ta) with a compression axis of [123] were subject to creep at a stress of 550 MPa and a temperature of 520 °C. Slip trace and TEM microstructural observations reveal that primary octahedral slip is responsible for the primary creep. In the secondary stage, cube cross slip (010) is operative. There is no obvious sign of inverse creep.