Hostname: page-component-7b7567c8c-p67k6 Total loading time: 0 Render date: 2026-11-19T10:18:50.458Z Has data issue: false hasContentIssue false

Deposition of Zinc Oxide Thin Films Using a Surface Reaction on Platinum Nanoparticles

Published online by Cambridge University Press:  05 April 2011

Kanji Yasui
Affiliation:
Nagaoka University of Technology, 1603-1 Kamitomioka, Nagaoka, Niigata 940-2188, Japan
Hitoshi Miura
Affiliation:
Nagaoka University of Technology, 1603-1 Kamitomioka, Nagaoka, Niigata 940-2188, Japan
Hiroshi Nishiyama
Affiliation:
Nagaoka University of Technology, 1603-1 Kamitomioka, Nagaoka, Niigata 940-2188, Japan
Get access

Abstract

A new chemical vapor deposition method for the growth of ZnO films using the reaction between dimethylzinc (DMZn) and thermally excited H2O produced by a Pt-catalyzed H2–O2 reaction was investigated. The thermally excited H2O molecules formed by the exothermic reaction of H2 and O2 on the catalyst were ejected from a fine nozzle into the reaction zone and allowed to collide with DMZn ejected from another fine nozzle. The ZnO films were grown directly on a-plane (11-20) sapphire substrates at substrate temperatures of 773-873 K with no buffer layer. X-ray diffraction patterns exhibited intense (0002) and (0004) peaks from the ZnO(0001) index plane. The smallest full width at half maximum (FWHM) value of the ω- rocking curve of ZnO(0002) was less than 0.1º. The largest Hall mobility and the smallest residual carrier concentration of the ZnO films were 169 cm2V−1s−1 and 1.7×1017 cm−3, respectively. Photoluminescence (PL) spectra at room temperature exhibited a band edge emission at 3.29 eV, with a FWHM of 104 meV. Green luminescence from deeper levels was generally about 1.5% of the band edge emission intensity. PL spectra at 5 K showed a strong emission peak at 3.3603 eV, attributed to the neutral donor-bound exciton Dºx. The FWHM was as low as 1.0 meV. Free exciton emissions also appeared at 3.3757 eV (FXA, n=1) and 3.4221 eV (FXA, n=2).

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2011

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable