Hostname: page-component-7b7567c8c-z4zkx Total loading time: 0 Render date: 2026-11-16T09:05:52.574Z Has data issue: false hasContentIssue false

Electrical Contacts to Polycrystalline B Doped Diamond Films

Published online by Cambridge University Press:  26 February 2011

K. Nishimura
Affiliation:
Visiting Scientist from Kobe Steel, Ltd., Japan
K. Das
Affiliation:
Department of Materials Science and Engineering, North Carolina State University, Raleigh, NC, 27695-7907
M. Iwase
Affiliation:
Visiting Scientist from Department of Engineering, Tokai University, 1117, Kitakanabe, Hiratsuka, Kanagawa, Japan, 259-12
J. T. Glass
Affiliation:
Department of Materials Science and Engineering, North Carolina State University, Raleigh, NC, 27695-7907
K. Kobashi
Affiliation:
Electronics Research Laboratory, Kobe Steel, Ltd., Takatsukadai 1-5-5, Nishiku, Kobe, Japan, 673-02
Get access

Abstract

B doped diamond films were synthesized by microwave plasma CVD and electrical contacts were fabricated by R F sputtering. Rc was obtained for Pt, Ni, TaSi2, and Al asdeposited contacts at room temperature. Pt gave the minimum Rc and Al gave the maximum Rc of the metals investigated on films containing a carrier concentration of 5 × 1018/cm3. The minimum Rc, 8.6 × 10−4 Ω cm 2, was obtained on heavily B doped diamond films with a carrier concentration of 2.7 × 1020/cm3. After nnealing at 400 °C, the Rc of Pt contacts on B doped diamond films with a resistivity of 2×104 Ω1 cm decreased by approximately one order of magnitude.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable