Hostname: page-component-7b7567c8c-7pwfn Total loading time: 0 Render date: 2026-11-17T00:31:49.085Z Has data issue: false hasContentIssue false

Evaluating Mechanical Properties of Thin Layers using Nanoindentation and Finite-Element Modeling: Implanted Metals and Deposited Layers

Published online by Cambridge University Press:  03 September 2012

J. A. Knapp
Affiliation:
Sandia National Laboratories, Albuquerque, NM 87185
D. M. Follstaedt
Affiliation:
Sandia National Laboratories, Albuquerque, NM 87185
J. C. Barbour
Affiliation:
Sandia National Laboratories, Albuquerque, NM 87185
S. M. Myers
Affiliation:
Sandia National Laboratories, Albuquerque, NM 87185
J. W. Ager
Affiliation:
Lawrence Berkeley National Laboratory, Berkeley, CA 94720
O. R. Monteiro
Affiliation:
Lawrence Berkeley National Laboratory, Berkeley, CA 94720
I. G. Brown
Affiliation:
Lawrence Berkeley National Laboratory, Berkeley, CA 94720
Get access

Abstract

We present a methodology based on finite-element modeling of nanoindentation data to extract reliable and accurate mechanical properties from thin, hard films and surface-modified layers on softer substrates. The method deduces the yield stress, Young's modulus, and hardness from indentations as deep as 50% of the layer thickness.