Hostname: page-component-7b7567c8c-2n9c9 Total loading time: 0 Render date: 2026-11-18T05:11:44.373Z Has data issue: false hasContentIssue false

Fabrication and Characterization of Electrically Functional Lanthanum Hexaboride Thin Films on Ultrasmooth Sapphire Substrates

Published online by Cambridge University Press:  01 February 2011

Yushi Kato
Affiliation:
kato.y.am@m.titech.ac.jp, Tokyo Institute of Technology, Department of Innovative & Engineered Materials, Yokohama, Japan
Yusaburo Ono
Affiliation:
ono.y.ad@m.titech.ac.jp, Tokyo Institute of Technology, Department of Innovative & Engineered Materials, Yokohama, Japan
Yasuyuki Akita
Affiliation:
akita.y.aa@m.titech.ac.jp, Tokyo Institute of Technology, Department of Innovative & Engineered Materials, Yokohama, Japan
Makoto Hosaka
Affiliation:
hosaka.m.ab@m.titech.ac.jp, Tokyo Institute of Technology, Department of Innovative & Engineered Materials, Yokohama, Japan
Naoki Shiraishi
Affiliation:
shiraishi.n.ab@m.titech.ac.jp, Tokyo Institute of Technology, Department of Innovative & Engineered Materials, Yokohama, Japan
Nobuo Tsuchimine
Affiliation:
tsuchimine@hotmail.com, TOSHIMA Manufacturing Company Limited, Saitama, Japan
Susumu Kobayashi
Affiliation:
Kobayashi@material-sys.com, TOSHIMA Manufacturing Company Limited, Saitama, Japan
Mamoru Yoshimoto
Affiliation:
yoshimoto.m.aa@m.titech.ac.jp, Tokyo Institute of Technology, Department of Innovative & Engineered Materials, Yokohama, Japan
Get access

Abstract

The crystal growth of lanthanum hexaboride (LaB6) thin films was examined by applying the laser molecular beam epitaxy (laser MBE) process. C-axis (100) highly-oriented LaB6 thin films could be fabricated on ultrasmooth sapphire (α-Al2O3 single crystal) (0001) substrates with atomic steps of 0.2 nm in height and atomically flat terraces. The obtained film exhibited a smooth surface with root mean square roughness of 0.15 nm. The lattice parameter of the LaB6 thin film was close to the bulk value reported previously. In the case of deposition on commercial mirror-polished sapphire substrates, the grown film was amorphous. The resistivity of the prepared crystalline LaB6 thin films was as low as 2.2 × 10−4 Ω cm and almost constant in the temperature range of 10–300 K.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable