Hostname: page-component-7b7567c8c-7pwfn Total loading time: 0 Render date: 2026-11-16T10:30:14.216Z Has data issue: false hasContentIssue false

Fracture Toughness and Subcritical Crack Growth in CVD Diamond

Published online by Cambridge University Press:  15 February 2011

A. Kant
Affiliation:
Materials Sciences Division, Lawrence Berkeley Laboratory, and Department of Materials Science and Mineral Engineering, University of California, Berkeley, CA 94720-1760
M. D. Drory
Affiliation:
Crystallume Corporation, Santa Clara, CA 95054
R. O. Ritchie
Affiliation:
Materials Sciences Division, Lawrence Berkeley Laboratory, and Department of Materials Science and Mineral Engineering, University of California, Berkeley, CA 94720-1760
Get access

Abstract

The fracture toughness, stress corrosion and cyclic fatigue properties of polycrystalline chemical vapor deposited (CVD) diamond have been investigated on thick (˜100 to 300 μm) free-standing films. Specifically, the fracture toughness, K c , of diamond was determined using indentation methods and for the first time by the tensile testing of pre-notched fracture-mechanics type compact-tension samples. Measured K c values were found to be between 5 and 7 MPa-m1/2 by either method and to be apparently independent of grain size and shape. Studies on subcritical crack growth (i.e., at stress intensities less than K c ) indicated that CVD diamond is essentially immune to stress-corrosion cracking under sustained loads in room air, water and acid environments. Corresponding experiments to examine susceptibility to cyclic fatigue are currently being performed using indentation-precracked cantilever beams cycled in three-point bending.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable