Growth Processes of Hydrogenated Amorphous Silicon

Published online by Cambridge University Press:  17 March 2011

John Robertson*
Affiliation:
Engineering Dept, Cambridge University, Cambridge CB2 1PZ, UK. jr@eng.cam.ac.uk
Get access

Abstract

The surface and subsurface processes occurring during the growth of a-Si:H are analysed to understand why dangling bond defects and weak Si-Si bonds form. We argue that hydrogen elimination to form the Si-Si network is the rate limiting process at low temperature, and this leads to the creation of weak Si-Si bonds. Dangling bonds form subsequently from weak bonds by a defect pool type process. Plasma processes, such as ion bombardment, which dehydrogenate the surface layers, can reduce the weak bond density.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable